Process for making structural gypsum board for neutron shielding

Assignee: Kaiser Gypsum Co Inc
•
Filing: 1963-11-12
•
Granted: 1969-07-01
•
Expires: 1983-11-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Arthur H Darling
  • 👤 Howard L Weightman

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 02:47
CPC Classifications
G; G21; G21F; G21F1/00; G21F1/02; C; C04; C04B; C04B28/00; C04B28/14; G21C; G21C11/00; G21C11/02; C04B2111/00; C04B2111/00474; C04B2111/00612; C04B2111/0062; C04B2111/00862; Y; Y02; Y02E; Y02E30/00; Y02E30/30

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 132 words
IN A METHOD OF FORMING A PAPER-LINED BOARD ADAPTED TO RESIST PASSAGE THERETHROUGH A NEUTRONS IMPINGING ON A SURFACE THEREOF, AND CONTAINING AS MAJOR PORTION A MASS OF SET GYPSUM CRYSTALS, THE STEPS WHICH COMPRISE CALCINING A RAW GYPSUM ROCK CONTAINING CALCIUM CARBONATE TO FORM CALCIUM SULFATE HEMI-HYDRATE CONTAINING SAID CARBONATE, INTIMATELY ADMIXING WITH SAID CALCINED MATERIAL FROM 4% TO 10% BORIC ACID EXPRESSED AS B2O3 AND BASED ON TOTAL WEIGHT OF SAID BORIC ACID PLUS SAID GYPSUM CRYSTALS, SEPARATELY INTIMATELY ADMIXING AN AMOUNT OF WATER AND AMMONIA, ADMIXING SAID AMMONIA-WATER MIXTURE WITH SAID CALCINED MATERIAL-BORIC ACID ADMIXTURE TO PREVENT EVOLUTION OF GAS AND TO FORM A PLASTIC SLURRY HAVING A PH OF FROM 6.0 TO 7.5, DEPOSITING SAID SLURRY BETWEEN A PAIR OF PAPER LINERS, FORMING INTO BOARD HARDENING AND DRYING.
Claim 2
Dependent Claim 132 words
IN A METHOD OF FORMING A PAPER-LINED BOARD ADAPTED TO RESIST PASSAGE THERETHROUGH A NEUTRONS IMPINGING ON A SURFACE THEREOF, AND CONTAINING AS MAJOR PORTION A MASS OF SET GYPSUM CRYSTALS, THE STEPS WHICH COMPRISE CALCINING A RAW GYPSUM ROCK CONTAINING CALCIUM CARBONATE TO FORM CALCIUM SULFATE HEMI-HYDRATE CONTAINING SAID CARBONATE, INTIMATELY ADMIXING WITH SAID CALCINED MATERIAL FROM 4% TO 10% BORIC ACID EXPRESSED AS B2O3 AND BASED ON TOTAL WEIGHT OF SAID BORIC ACID PLUS SAID GYPSUM CRYSTALS, SEPARATELY INTIMATELY ADMIXING AN AMOUNT OF WATER AND AMMONIA, ADMIXING SAID AMMONIA-WATER MIXTURE WITH SAID CALCINED MATERIAL-BORIC ACID ADMIXTURE TO PREVENT EVOLUTION OF GAS AND TO FORM A PLASTIC SLURRY HAVING A PH OF FROM 6.0 TO 7.5, DEPOSITING SAID SLURRY BETWEEN A PAIR OF PAPER LINERS, FORMING INTO BOARD HARDENING AND DRYING.

References Cited (Backward Citations)

US3043298A Cited
US3126352A Cited
US3181985A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1972-06-30 1972-12-30 1973-07-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1976-06-30 1976-12-30 1977-07-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1980-06-30 1980-12-30 1981-07-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag