← Back to Patent Explorer
US3331657A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of preventing the depositing of sulfur in the riser pipes in producing natural gases laden with hydrogen sulfide and containing elemental sulfur in solution

Assignee: Gewerkschaft Elwerath
•
Filing: 1963-04-03
•
Granted: 1967-07-18
•
Expires: 1983-04-03
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Peter Siegfried
  • 👤 Buchholz Otto

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 09:57
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/52; C09K8/528; C09K8/532; C01; C01B; C01B17/00; C01B17/22; C01B17/34; C01C; C01C1/00; C01C1/20; C10; C10K; C10K1/00; C10K1/08; C10K1/10; C10K1/12; C10K1/121; C10K1/122

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 149 words
IN A METHOD OF PREVENTING THE FORMATION FO SOLID SULFUR IN A STREAM OF NATURAL GAS DURING UPWARD PASSAGE OF THE SAME FROM A SUBTERRANEAN NATURAL GAS DEPOSIT, SAID NATURAL GAS INCLUDING H2S, CO2 AND ELEMENTARY SULFUR AND BEING INITIALLY AT AN ELEVATED PRESSURE, AND TEMPERATURE SUFFICIENTLY HIGH TO MAINTAIN SAID SULFUR IN SOLUTION IN SAID H2S, THE STEP OF INTRODUCING INTO SAID STREAM OF NATURAL GAS DURING UPWARD PASSAGE OF THE SAME, AT A POINT AT WHICH THE PRESSURE AND TEMPERATURE OF SAID NATURAL GAS STREAM ARE STILL SUFFICIENTLY HIGH TO MAINTAIN SAID SULFUR IN SOLUTION IN SAID H2S, AN AQUEOUS SOLUTION OF THE HYDROXIDE OF AT LEAST ONE SUBSTANCE SELECTED FROM THE GROUP CONSISTING OF ALKALI METALS AND AMMONIA SO AS TO FORM AN AQUEOUS SOLUTION OF THE SULFIDE OF SAID SUBSTANCE HAVING SAID SULFUR DISSOLVED THEREIN IN THE FORM OF AN ALKAI METAL OR AMMONIUM POLYSULFIDE.
Claim 2
Dependent Claim 149 words
IN A METHOD OF PREVENTING THE FORMATION FO SOLID SULFUR IN A STREAM OF NATURAL GAS DURING UPWARD PASSAGE OF THE SAME FROM A SUBTERRANEAN NATURAL GAS DEPOSIT, SAID NATURAL GAS INCLUDING H2S, CO2 AND ELEMENTARY SULFUR AND BEING INITIALLY AT AN ELEVATED PRESSURE, AND TEMPERATURE SUFFICIENTLY HIGH TO MAINTAIN SAID SULFUR IN SOLUTION IN SAID H2S, THE STEP OF INTRODUCING INTO SAID STREAM OF NATURAL GAS DURING UPWARD PASSAGE OF THE SAME, AT A POINT AT WHICH THE PRESSURE AND TEMPERATURE OF SAID NATURAL GAS STREAM ARE STILL SUFFICIENTLY HIGH TO MAINTAIN SAID SULFUR IN SOLUTION IN SAID H2S, AN AQUEOUS SOLUTION OF THE HYDROXIDE OF AT LEAST ONE SUBSTANCE SELECTED FROM THE GROUP CONSISTING OF ALKALI METALS AND AMMONIA SO AS TO FORM AN AQUEOUS SOLUTION OF THE SULFIDE OF SAID SUBSTANCE HAVING SAID SULFUR DISSOLVED THEREIN IN THE FORM OF AN ALKAI METAL OR AMMONIUM POLYSULFIDE.

References Cited (Backward Citations)

US1360734A Cited
US1771293A Cited
US1837493A Cited
US2688368A Cited
US3097917A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1970-07-17 1971-01-16 1971-07-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1974-07-17 1975-01-16 1975-07-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1978-07-17 1979-01-16 1979-07-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag