← Back to Patent Explorer
US3296179A Expired / Lapsed US ⏱️ 0.0 years remaining

Epoxidized polymer of butadiene cured with oxalic or malonic acid at room temperature

Assignee: FMC Corp
•
Filing: 1963-03-25
•
Granted: 1967-01-03
•
Expires: 1983-03-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Lister Fred
  • 👤 Charles G Cullen
  • 👤 Theodore R Hopper

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 13:23
CPC Classifications
C; C08; C08G; C08G59/00; C08G59/02; C08G59/027; C08C; C08C19/00; C08C19/30; C08C19/34; C08C19/40; C08G59/18; C08G59/40; C08G59/42; C08G59/4207

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 112 words
A METHOD OF CURING AN EPOXIDIZED POLYMER OF BUTADIENE AT ROOM TEMPERATURE TO A HARD, TOUGH, ADHERENT AND SOLVENT AND CHEMICAL REISTANT FILM WHICH COMPRISES: MIXING (A) AN EPOXIDIZED POLYMER OF BUADIENE HAVIGN AN OXIRANE OXYGEN CONTENT OF 6-12% BY WEIGHT IN WHICH 60-100% OF THE POLYMER FORMING UNITS ARE DERIVED FROM BUTADIENE AND THE BALANCE FROM AN ETHYLENICALLY UNSATURATED COMNOMER AND (B) A VOLATILE ORGANIC SOLVENT SOLUTION OF A DICARBOXYLIC ACID SELECTED FROM THE GROUP CONSISTING OF OXALIC ACID AND MALONIC ACID CONTAINING 0.05-0.4 MOLE OF DICARBOXYLIC ACID PER OXIRANE EQUIVALENT OF EPOXIDIZED POLYMER OF BUTADIENE, APPLYING THE MIXTURE AS A COATING, AND ALLOWING THE COATING TO CURE AT ROOM TEMPERATURE.
Claim 2
Independent Claim 112 words
A METHOD OF CURING AN EPOXIDIZED POLYMER OF BUTADIENE AT ROOM TEMPERATURE TO A HARD, TOUGH, ADHERENT AND SOLVENT AND CHEMICAL REISTANT FILM WHICH COMPRISES: MIXING (A) AN EPOXIDIZED POLYMER OF BUADIENE HAVIGN AN OXIRANE OXYGEN CONTENT OF 6-12% BY WEIGHT IN WHICH 60-100% OF THE POLYMER FORMING UNITS ARE DERIVED FROM BUTADIENE AND THE BALANCE FROM AN ETHYLENICALLY UNSATURATED COMNOMER AND (B) A VOLATILE ORGANIC SOLVENT SOLUTION OF A DICARBOXYLIC ACID SELECTED FROM THE GROUP CONSISTING OF OXALIC ACID AND MALONIC ACID CONTAINING 0.05-0.4 MOLE OF DICARBOXYLIC ACID PER OXIRANE EQUIVALENT OF EPOXIDIZED POLYMER OF BUTADIENE, APPLYING THE MIXTURE AS A COATING, AND ALLOWING THE COATING TO CURE AT ROOM TEMPERATURE.

References Cited (Backward Citations)

US2500449A Cited
US2829135A Cited
US2949441A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1970-01-02 1970-07-04 1971-01-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1974-01-02 1974-07-04 1975-01-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1978-01-02 1978-07-04 1979-01-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags