US3290180A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of treating silicon and devices containing pn junctions

Assignee: Texas Instruments Inc
•
Filing: 1965-04-05
•
Granted: 1966-12-06
•
Expires: 1985-04-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Stephen S Baird
  • 👤 Clyde R Fuller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 05:13
CPC Classifications
H; H10; H10P; H10P70/00; H10P70/10; H10P70/15; H10P14/00; H10P14/60; H10P14/63; H10P14/6302; H10P14/6304; H10P14/6306; H10P14/6308; H10P14/6309; H10P14/6322; H10P14/65; H10P14/6502; H10P14/6508; H10W; H10W74/00; H10W74/40; H10W74/47; Y; Y10; Y10S; Y10S148/00; Y10S148/003; Y10S148/017; Y10S148/118; Y10S438/00; Y10S438/906

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 131 words
THE METHOD OF PREPARING A PROTECTED SILICON PN JUNCTION WHICH COMPRISES THE STEPS OF DEGREASING THE SILICON SLICE IN TRICHLOROETHYLENE, RINSING IT IN METHYL ALCOHOL AND WATER, BOILING IT FOR 20 MINUTES AT 100*C. IN NITRIC ACID, RINSING IT IN DEIONIZED WATER FOR 5 MINUTES, HEATING IT IN CONCENTRATED SULFURIC ACID AT 200*C. FOR 20 MINUTES AND RINSING IN DEIONIZED RUNNING WATER FOR 5 MINUTES, SOAKING IN HYDROFLUORIC ACID FOR 30 MINUTES AND RINSING IN WATER 5 MINUTES, BOILING IN DEIONIZED WATER TWICE FOR 15 MINUTES AND RINSING IN WATER 5 MINUTES, BOILING IN NITRIC ACID 30 MINUTES AND RINSING IN DEIONIZED RUNNING WATER FOR 30 MINUTES, OXIDIZING ABOUT FIVE AND ONEHALF HOURS IN STREAM AT ATMOSPHERIC PRESSURE AT 1200*C., DRYING IN HELIUM FOR ONE HOUR AND COOLING TO ROOM TEMPERATURE.
Claim 2
Independent Claim 131 words
THE METHOD OF PREPARING A PROTECTED SILICON PN JUNCTION WHICH COMPRISES THE STEPS OF DEGREASING THE SILICON SLICE IN TRICHLOROETHYLENE, RINSING IT IN METHYL ALCOHOL AND WATER, BOILING IT FOR 20 MINUTES AT 100*C. IN NITRIC ACID, RINSING IT IN DEIONIZED WATER FOR 5 MINUTES, HEATING IT IN CONCENTRATED SULFURIC ACID AT 200*C. FOR 20 MINUTES AND RINSING IN DEIONIZED RUNNING WATER FOR 5 MINUTES, SOAKING IN HYDROFLUORIC ACID FOR 30 MINUTES AND RINSING IN WATER 5 MINUTES, BOILING IN DEIONIZED WATER TWICE FOR 15 MINUTES AND RINSING IN WATER 5 MINUTES, BOILING IN NITRIC ACID 30 MINUTES AND RINSING IN DEIONIZED RUNNING WATER FOR 30 MINUTES, OXIDIZING ABOUT FIVE AND ONEHALF HOURS IN STREAM AT ATMOSPHERIC PRESSURE AT 1200*C., DRYING IN HELIUM FOR ONE HOUR AND COOLING TO ROOM TEMPERATURE.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-12-05 1970-06-06 1970-12-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-12-05 1974-06-06 1974-12-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-12-05 1978-06-06 1978-12-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag