Abstract

No abstract record available.

Inventors

  • 👤 Victor G Reiling

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 04:41
CPC Classifications
C; C08; C08L; C08L27/00; C08L27/02; C08L27/12; C08L27/18

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 126 words
A COMPOSITION OF MATTER CONSISTING ESSENTIALLY OF FINELY DIVIDED DEGRADED POLYTETRAFLUOROETHYLENE RESIN PARTICLES AND A PARENT MATERIAL THEREFOR, SAID PARENT MATERIAL BEING SELECTED FROM THE GROUP CONSISTING OF THERMOSETTING AND THERMOPLASTIC RESINS AND COMBINATIONS THEREOF, SAID DEGRADED POLYTETRAFLUOROETHYLENE RESIN BEING FORMED BY HEATING POLYTETRAFLUOROETHYLENE RESIN STARTING MATERIAL AT A TEMPERATURE IN EXCESS OF 785*F. FOR A PERIOD OF TIME SUFFICIENT TO CAUSE APPRECIABLE DEGRADATION OF SAID POLYTETRAFLUOROETHYLENE STARTING MATERIAL TO A POINT SUCH THAT THE TENSILE STRENGTH OF THE DEGRADED POLYTETRAFLUOROETHYLENE IS PERMANENTLY SUBSTANTIALLY LESS THAN THAT OF THE STARTING MATERIAL, AND SAID DEGRADED RESIN PARTICLES BEING PRESENT IN AN AMOUNT OF 5 TO 50% BY VOLLUME OF SAID PARENT RESIN AND BEING UNIFORMLY AND EVENLY DISTRIBUTED THROUGHOUT SAID PARENT FOR REDUCING THE SURFACE FRICTION THEREOF.
Claim 2
Dependent Claim 126 words
A COMPOSITION OF MATTER CONSISTING ESSENTIALLY OF FINELY DIVIDED DEGRADED POLYTETRAFLUOROETHYLENE RESIN PARTICLES AND A PARENT MATERIAL THEREFOR, SAID PARENT MATERIAL BEING SELECTED FROM THE GROUP CONSISTING OF THERMOSETTING AND THERMOPLASTIC RESINS AND COMBINATIONS THEREOF, SAID DEGRADED POLYTETRAFLUOROETHYLENE RESIN BEING FORMED BY HEATING POLYTETRAFLUOROETHYLENE RESIN STARTING MATERIAL AT A TEMPERATURE IN EXCESS OF 785*F. FOR A PERIOD OF TIME SUFFICIENT TO CAUSE APPRECIABLE DEGRADATION OF SAID POLYTETRAFLUOROETHYLENE STARTING MATERIAL TO A POINT SUCH THAT THE TENSILE STRENGTH OF THE DEGRADED POLYTETRAFLUOROETHYLENE IS PERMANENTLY SUBSTANTIALLY LESS THAN THAT OF THE STARTING MATERIAL, AND SAID DEGRADED RESIN PARTICLES BEING PRESENT IN AN AMOUNT OF 5 TO 50% BY VOLLUME OF SAID PARENT RESIN AND BEING UNIFORMLY AND EVENLY DISTRIBUTED THROUGHOUT SAID PARENT FOR REDUCING THE SURFACE FRICTION THEREOF.

References Cited (Backward Citations)

US2400091A Cited
US2847711A Cited
US2998397A Cited
US2933536A Cited
US3005795A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-11-21 1970-05-23 1970-11-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-11-21 1974-05-23 1974-11-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-11-21 1978-05-23 1978-11-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag