Method of removing insulating material from electrical conductors

Assignee: Methode Electronics Inc
•
Filing: 1963-07-19
•
Granted: 1966-09-27
•
Expires: 1983-07-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Duane A Schroeder

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 16:41
CPC Classifications
H; H05; H05K; H05K3/00; H05K3/0011; H05K3/0017; H05K3/002; H02; H02G; H02G1/00; H02G1/12; H02G1/1287; H05K2201/00; H05K2201/01; H05K2201/0137; H05K2201/0145; H05K2203/00; H05K2203/07; H05K2203/0779; H05K2203/0786; H05K2203/0789; H05K3/40; H05K3/4092

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 157 words
THE PROCESS OF REMOVING POLYESTER INSULATING MATERIAL FROM COPPER CONDUCTIVE ELEMENTS OF A FLEXIBLE WIRING UNIT LEAVING A CLEAN, SHARP END MARGIN ON THE REMAINING POLYESTER MATERIAL WHICH COMPRISES: (A) MASKING AN AREA OF A FLEXIBLE WIRING UNIT FORMED BY COPPER CONDUCTIVE ELEMENTS ENCAPSULATED IN POLYESTER INSULATING MATERIAL ADJACENT THE INTENDED POINTS OF ELECTRICAL CONTACT WITH LEAD FOIL HAVING ONE OF ITS FACES COATED WITH A PRESSURE SENSITIVE ADHESIVE BY PLACING THE ADHESIVE SURFACE OF THE MASKING FOIL AGAINST THE POLYESTER AND PRESSING THE FOIL INTO INTIMATE CONTACT WITH THE SURFACE OF SAID UNIT. (B) FLOODING THE AREA OF POLYESTER TO BE REMOVED WITH SULFURIC ACID HAVING A CONCENTRATION OF BETWEEN ABOUT 1.53 TO 1.84*BE. AT A TEMPERATURE OF BETWEEN 135* F. AND THE BOILING POINT OF THE ACID. (C) REMOVING THE UNIT FORM CONTACT WITH SAID ACID BEFORE DELECTERIOUS ATTACH ON THE LEAD AND COPPER BEGINS, (D) NEUTRALIZING ANY ADHERENT ACID AND DRYING THE UNIT, AND
Claim 2
Dependent Claim 157 words
THE PROCESS OF REMOVING POLYESTER INSULATING MATERIAL FROM COPPER CONDUCTIVE ELEMENTS OF A FLEXIBLE WIRING UNIT LEAVING A CLEAN, SHARP END MARGIN ON THE REMAINING POLYESTER MATERIAL WHICH COMPRISES: (A) MASKING AN AREA OF A FLEXIBLE WIRING UNIT FORMED BY COPPER CONDUCTIVE ELEMENTS ENCAPSULATED IN POLYESTER INSULATING MATERIAL ADJACENT THE INTENDED POINTS OF ELECTRICAL CONTACT WITH LEAD FOIL HAVING ONE OF ITS FACES COATED WITH A PRESSURE SENSITIVE ADHESIVE BY PLACING THE ADHESIVE SURFACE OF THE MASKING FOIL AGAINST THE POLYESTER AND PRESSING THE FOIL INTO INTIMATE CONTACT WITH THE SURFACE OF SAID UNIT. (B) FLOODING THE AREA OF POLYESTER TO BE REMOVED WITH SULFURIC ACID HAVING A CONCENTRATION OF BETWEEN ABOUT 1.53 TO 1.84*BE. AT A TEMPERATURE OF BETWEEN 135* F. AND THE BOILING POINT OF THE ACID. (C) REMOVING THE UNIT FORM CONTACT WITH SAID ACID BEFORE DELECTERIOUS ATTACH ON THE LEAD AND COPPER BEGINS, (D) NEUTRALIZING ANY ADHERENT ACID AND DRYING THE UNIT, AND

References Cited (Backward Citations)

GB730958A Cited
US2979387A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-09-26 1970-03-28 1970-09-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-09-26 1974-03-28 1974-09-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-09-26 1978-03-28 1978-09-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag