Overlay welding

Assignee: Hoskins Manufacturing Co
•
Filing: 1965-06-24
•
Granted: 1966-09-06
•
Expires: 1985-06-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Wallace C Johnson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 10:44
CPC Classifications
B; B23; B23K; B23K9/00; B23K9/04; B23K2101/00; B23K2101/04; B23K2101/06; Y; Y10; Y10T; Y10T29/00; Y10T29/51

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 159 words
A PROCESS OF OVERLAY WELDING ON A BASE METAL WHICH HAS WELDED THERETO A PREVIOUS OVERLAY WELD BEAD EXTENDING LENGTHSWISE ALONG ONE SURFACE OF THE BASE METAL, WHICH COMPRISES LAYING DOWN A CONSUMABLE BARRIER STRIP ADJOINING THE EDGE OF THE PREVIOUS WELD BEAD AND AGAINST THE SURFACE OF THE BASE METAL, SAID BARRIER STRIP BEING WIDER THAN IT IS THICK AND THE THICKNESS OF THE BARRIER STRIP EXTENDING TRANSVERSELY TO THE SURFACE OF THE BASE METAL, ARCING FROM A STRIP ELECTRODE WHICH IS WIDER THAN IT IS THICK AND WHICH OVERHANGS THE BARRIER STRIP AND OVERHANGS THE EDGE OF THE PREVIOUS WELD BEAD, TO A WELD POOL FORMED BY MELTING ALL OF THE BARRIER STRIP, ALL OF THE STRIP ELECTRODE, THE EDGE OF THE PREVIOUS WELD BEAD AND THE SURFACE OF THE BASE METAL, AND ADVANCING THE STRIP ELECTRODE IN THE DIRECTION OF ITS THICKNESS LENGTHWISE OF THE BARRIER STRIP AND THE ADJOINING EDGE OF THE PREVIOUS WELD BEAD.
Claim 2
Dependent Claim 159 words
A PROCESS OF OVERLAY WELDING ON A BASE METAL WHICH HAS WELDED THERETO A PREVIOUS OVERLAY WELD BEAD EXTENDING LENGTHSWISE ALONG ONE SURFACE OF THE BASE METAL, WHICH COMPRISES LAYING DOWN A CONSUMABLE BARRIER STRIP ADJOINING THE EDGE OF THE PREVIOUS WELD BEAD AND AGAINST THE SURFACE OF THE BASE METAL, SAID BARRIER STRIP BEING WIDER THAN IT IS THICK AND THE THICKNESS OF THE BARRIER STRIP EXTENDING TRANSVERSELY TO THE SURFACE OF THE BASE METAL, ARCING FROM A STRIP ELECTRODE WHICH IS WIDER THAN IT IS THICK AND WHICH OVERHANGS THE BARRIER STRIP AND OVERHANGS THE EDGE OF THE PREVIOUS WELD BEAD, TO A WELD POOL FORMED BY MELTING ALL OF THE BARRIER STRIP, ALL OF THE STRIP ELECTRODE, THE EDGE OF THE PREVIOUS WELD BEAD AND THE SURFACE OF THE BASE METAL, AND ADVANCING THE STRIP ELECTRODE IN THE DIRECTION OF ITS THICKNESS LENGTHWISE OF THE BARRIER STRIP AND THE ADJOINING EDGE OF THE PREVIOUS WELD BEAD.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-09-05 1970-03-07 1970-09-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-09-05 1974-03-07 1974-09-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-09-05 1978-03-07 1978-09-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag