Abstract

No abstract record available.

Inventors

  • 👤 Quinn James Maurice

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 16:42
CPC Classifications
C; C08; C08L; C08L27/00; B; B29; B29C; B29C55/00; B29C59/00; B65; B65D; B65D35/00; B65D35/02; C08J; C08J5/00; C08J5/18; C08L27/02; C08L27/04; C08L27/06; C08J2327/00; C08J2327/02; C08J2327/04; C08J2327/06; Y; Y02; Y02A; Y02A40/00; Y02A40/90; Y02W; Y02W90/00; Y02W90/10

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 131 words
A PROCESS OF PREPARING POLYVINYL CHLORIDE FILM WHICH COMPRISES THE STEPS IN SQUENCE OF EXTRUDING A MELT CONTAINING POLYVINYL CHLORIDE RESIN AND ADDITIVES COMPRISING A HEAT-STABILIZING AGENT AT LEAST ONE OF SAID ADDITIVES HAVING PLASTICIZING PROPERTIES, THE TOTAL AMOUNT OF ADDITIVES BEING SUCH AS TO PRODUCE AN EFFECT O GREATER THAN THAT PRODUCED BY 1.5 TO 10% OF A PRIMARY PLASTICIZER FOR SAID RESIN TO FORM A FILM; ELONGATING SAID FILM IN AT LEAST ONE DIRECTION AN AMOUNT NECESSARY TO INCREASE THE PLANAR ORIENTATION NUMBER OF SAID FILM TO AT LEAST 16 WHILE HOLDING SAID FILM AT A TEMPERATURE OF 80-115*C.; AND, THEREAFTER, COOLING SAID FILM TO A TEMPERATURE BELOW 70*C. WHILE IMPOSING TENSION ON SAID FILM TO PREVENT ANY SUBSTANTIAL CHANGE IN THE FILM''S DIMENSIONS; AND THEREAFTER, RELEASING SAID TENSION.
Claim 2
Dependent Claim 131 words
A PROCESS OF PREPARING POLYVINYL CHLORIDE FILM WHICH COMPRISES THE STEPS IN SQUENCE OF EXTRUDING A MELT CONTAINING POLYVINYL CHLORIDE RESIN AND ADDITIVES COMPRISING A HEAT-STABILIZING AGENT AT LEAST ONE OF SAID ADDITIVES HAVING PLASTICIZING PROPERTIES, THE TOTAL AMOUNT OF ADDITIVES BEING SUCH AS TO PRODUCE AN EFFECT O GREATER THAN THAT PRODUCED BY 1.5 TO 10% OF A PRIMARY PLASTICIZER FOR SAID RESIN TO FORM A FILM; ELONGATING SAID FILM IN AT LEAST ONE DIRECTION AN AMOUNT NECESSARY TO INCREASE THE PLANAR ORIENTATION NUMBER OF SAID FILM TO AT LEAST 16 WHILE HOLDING SAID FILM AT A TEMPERATURE OF 80-115*C.; AND, THEREAFTER, COOLING SAID FILM TO A TEMPERATURE BELOW 70*C. WHILE IMPOSING TENSION ON SAID FILM TO PREVENT ANY SUBSTANTIAL CHANGE IN THE FILM''S DIMENSIONS; AND THEREAFTER, RELEASING SAID TENSION.

References Cited (Backward Citations)

US2952867A Cited
US2851733A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-05-30 1969-11-29 1970-05-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-05-30 1973-11-29 1974-05-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-05-30 1977-11-29 1978-05-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags