Stable slurry of calcium carbonate and calcium stearate, and methods of making and using it

Assignee: ExxonMobil Technology and Engineering Co
•
Filing: 1961-12-28
•
Granted: 1966-05-31
•
Expires: 1981-12-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Jr William G De Pierri

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 15:27
CPC Classifications
C; C08; C08K; C08K3/00; C08K3/18; C08K3/24; C08K3/26; C08K5/00; C08K5/04; C08K5/09; C08K5/098

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 112 words
A METHOD OF ADDING CALCIUM CARBONATE AND CALCIUM STEARATE TO A POLYOLEFIN PRODUCT TO IMPROVE THE MOLD CORROSION AND OXIDATIVE STABILITY THEREOF WHICH COMPRISES ADMIXING IN A MIXING ZONE 100 PARTS BY WEIGHT OF CALCIUM CARBONATE PARTICLES HAVING A MAXIUM SIZE OF 15 MICRONS WITH FROM 50 TO 500 PARTS OF CALCIUM STEARATE PARTICLES HAVING A MAXIMUM SIZE OF 50 MICRONS AND SUFFICIENT SOLVENT TO PRODUCE A SLURRY HAVING A MAXIMUM SOLIDS CONTENT OF 40% BY WEIGHT, SAID ADMIXING BEING CONTINUED FOR A TIME SUFFICIENT TO FORM A HOMOGENEOUS SLURRY, AND ADMIXING SAID SLURRY WITH SAID POLYOLEFIN WHICH IS RECOVERED FROM THE POLYMERIZATION REACTION AND BEFORE SAID POLYOLEFIN HAS BEEN COMPLETELY DRIED.
Claim 2
Independent Claim 112 words
A METHOD OF ADDING CALCIUM CARBONATE AND CALCIUM STEARATE TO A POLYOLEFIN PRODUCT TO IMPROVE THE MOLD CORROSION AND OXIDATIVE STABILITY THEREOF WHICH COMPRISES ADMIXING IN A MIXING ZONE 100 PARTS BY WEIGHT OF CALCIUM CARBONATE PARTICLES HAVING A MAXIUM SIZE OF 15 MICRONS WITH FROM 50 TO 500 PARTS OF CALCIUM STEARATE PARTICLES HAVING A MAXIMUM SIZE OF 50 MICRONS AND SUFFICIENT SOLVENT TO PRODUCE A SLURRY HAVING A MAXIMUM SOLIDS CONTENT OF 40% BY WEIGHT, SAID ADMIXING BEING CONTINUED FOR A TIME SUFFICIENT TO FORM A HOMOGENEOUS SLURRY, AND ADMIXING SAID SLURRY WITH SAID POLYOLEFIN WHICH IS RECOVERED FROM THE POLYMERIZATION REACTION AND BEFORE SAID POLYOLEFIN HAS BEEN COMPLETELY DRIED.
Claim 3
Independent Claim 64 words
A METHOD OF FORMING A STABLE SLURRY FOR ADDITION TO A POLYOLEFIN PRODUCT WHICH COMPRISES ADMIXING 100 PARTS OF WEIGHT OF CALCIUM CARBONATE HAVING A MAXIMUM SIZE OF 15 MICRONS WITH 50 TO 500 PARTS BY WEIGHT OF CALCIUM STEARATE HAVING A MAXIMUM PARTICLE SIZE OF 50 MICRONS, AND SUFFICIENT SOLVENT TO PRODUCE A SLURRY HAVING A MAXIMUM SOLIDS CONTENT OF 40% BY WEIGHT.
Claim 4
Independent Claim 64 words
A METHOD OF FORMING A STABLE SLURRY FOR ADDITION TO A POLYOLEFIN PRODUCT WHICH COMPRISES ADMIXING 100 PARTS OF WEIGHT OF CALCIUM CARBONATE HAVING A MAXIMUM SIZE OF 15 MICRONS WITH 50 TO 500 PARTS BY WEIGHT OF CALCIUM STEARATE HAVING A MAXIMUM PARTICLE SIZE OF 50 MICRONS, AND SUFFICIENT SOLVENT TO PRODUCE A SLURRY HAVING A MAXIMUM SOLIDS CONTENT OF 40% BY WEIGHT.

References Cited (Backward Citations)

US2863784A Cited
US2883901A Cited
US2985617A Cited
US2984634A Cited
US2990748A Cited
US2991264A Cited
US3160598A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-05-30 1969-11-29 1970-05-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-05-30 1973-11-29 1974-05-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-05-30 1977-11-29 1978-05-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag