← Back to Patent Explorer
US3252875A Expired / Lapsed US ⏱️ 0.0 years remaining

Aluminum anodizing method

Assignee: Alcoa Corp
•
Filing: 1961-11-09
•
Granted: 1966-05-24
•
Expires: 1981-11-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Economy George

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 13:32
CPC Classifications
C; C25; C25D; C25D11/00; C25D11/02; C25D11/04; C25D11/14

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 117 words
A METHOD OF ANODIZING ALUMINUM, COMPRISING MAKING AN ALUMINUM ARTICLE ANODE IN AN ELECTROLYTE CONSISTING ESSENTIALLY OF AT LEAST 10 GRAMS PER LITER OF OXALIC ACID (CALCULATED AS HO2C.CO2H.2H2O), AT LEAST 1/4 GRAM PERLITER OF SULFATE (CALCULATED AS H2SO4) PROVIDED BY AT LEAST ONE COMPOUND SELECTED FROM THE GROUP CONSISTING OF SULFURIC ACID AND WATER SOLUBLE SULFATES AND BISULFATES, AND WATER, THE WEIGHT RATION (R) OF SAID OXALIC ACID TO SAID SULFATE BEING AT LEAST THAT EXPRESSED BY THE FORMULA: R=21-2/15T, WHERE T IS THE ELECTROLYTE TEMPERATURE IN *F., WHILE THE ELECTROLYTE IS MAINTAINED AT A TEMPEATURE BETWEEN ABOUT 55 AND 90*F., FOR A TIME OF TREATMENT SUFFICIENT TO PRODUCE AN ANODIC OXIDE COATING OF SUBSTANTIAL THICKNESS.
Claim 2
Independent Claim 117 words
A METHOD OF ANODIZING ALUMINUM, COMPRISING MAKING AN ALUMINUM ARTICLE ANODE IN AN ELECTROLYTE CONSISTING ESSENTIALLY OF AT LEAST 10 GRAMS PER LITER OF OXALIC ACID (CALCULATED AS HO2C.CO2H.2H2O), AT LEAST 1/4 GRAM PERLITER OF SULFATE (CALCULATED AS H2SO4) PROVIDED BY AT LEAST ONE COMPOUND SELECTED FROM THE GROUP CONSISTING OF SULFURIC ACID AND WATER SOLUBLE SULFATES AND BISULFATES, AND WATER, THE WEIGHT RATION (R) OF SAID OXALIC ACID TO SAID SULFATE BEING AT LEAST THAT EXPRESSED BY THE FORMULA: R=21-2/15T, WHERE T IS THE ELECTROLYTE TEMPERATURE IN *F., WHILE THE ELECTROLYTE IS MAINTAINED AT A TEMPEATURE BETWEEN ABOUT 55 AND 90*F., FOR A TIME OF TREATMENT SUFFICIENT TO PRODUCE AN ANODIC OXIDE COATING OF SUBSTANTIAL THICKNESS.

References Cited (Backward Citations)

US1965682A Cited
US2998358A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-05-23 1969-11-22 1970-05-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-05-23 1973-11-22 1974-05-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-05-23 1977-11-22 1978-05-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag