← Back to Patent Explorer
US3220993A Expired / Lapsed US ⏱️ 0.0 years remaining

Halogenated dehydropolycyclopentadiene and its preparation

Assignee: ExxonMobil Oil Corp
•
Filing: 1962-09-27
•
Granted: 1965-11-30
•
Expires: 1982-09-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Paul E Blatz

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 06:37
CPC Classifications
C; C08; C08F; C08F8/00; C08F8/18; C08F8/20; C08F8/22

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 32 words
A SOLID HALOGENTAED DEHYDROPOLYCYCLOPENTADIENE CONSISTING SUBSTNAITALLY OF A LINEAR SERIES OF FIVE-MEMBERED RINGS AND CONTAINING FROM ABOUT ONE TO ABOUT THREE ATOMS OF A HALOGEN PER SIX FIVE-MEMBERED RINGS IN SAID POLYMER.
Claim 2
Dependent Claim 32 words
A SOLID HALOGENTAED DEHYDROPOLYCYCLOPENTADIENE CONSISTING SUBSTNAITALLY OF A LINEAR SERIES OF FIVE-MEMBERED RINGS AND CONTAINING FROM ABOUT ONE TO ABOUT THREE ATOMS OF A HALOGEN PER SIX FIVE-MEMBERED RINGS IN SAID POLYMER.
Claim 3
Independent Claim 89 words
A METHOD FOR PREPARATION OF A SOLID HALOGENATED DEHYDROPLYCYCLOPENTADIENE WHICH COMPRISES CONTRACTING A SOLUTION OF A SOLID POLYMER OF CYCLOPENTADIENE WITH A HALOGEN TO INITIALLY PRODUCE A HALOGENATED POLYCYCLOPENTADIENE CONTAINING SUBSTANTIALLY MORE THAN ONE ATOM OF HALOGEN PER TWO FIVE-MEMBERED RINGS IN THE POLYMER AND HEATING SAID HALOGENATED POLYCYCLOPENTADIENE AT FROM ABOUT 40 TO ABOUT 100*C. FOR AT LEAST ABOUT ONE HALF HOUR TO DEHALOGENATE SAID HALOGENATED POLYCYCLOPENTADIENE TO A SOLID POLYMER CONTAINING FROM ABOUT ONE TO ABOUT THREE ATOMS OF HALOGEN PER SIX FIVE-MEMBERED RINGS IN SAID POLYMER.
Claim 4
Independent Claim 89 words
A METHOD FOR PREPARATION OF A SOLID HALOGENATED DEHYDROPLYCYCLOPENTADIENE WHICH COMPRISES CONTRACTING A SOLUTION OF A SOLID POLYMER OF CYCLOPENTADIENE WITH A HALOGEN TO INITIALLY PRODUCE A HALOGENATED POLYCYCLOPENTADIENE CONTAINING SUBSTANTIALLY MORE THAN ONE ATOM OF HALOGEN PER TWO FIVE-MEMBERED RINGS IN THE POLYMER AND HEATING SAID HALOGENATED POLYCYCLOPENTADIENE AT FROM ABOUT 40 TO ABOUT 100*C. FOR AT LEAST ABOUT ONE HALF HOUR TO DEHALOGENATE SAID HALOGENATED POLYCYCLOPENTADIENE TO A SOLID POLYMER CONTAINING FROM ABOUT ONE TO ABOUT THREE ATOMS OF HALOGEN PER SIX FIVE-MEMBERED RINGS IN SAID POLYMER.

References Cited (Backward Citations)

US2261757A Cited
US2513330A Cited
US2581927A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-11-29 1969-05-31 1969-11-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-11-29 1973-05-31 1973-11-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-11-29 1977-05-31 1977-11-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag