Method of treating chrysotile and product produced thereby

Assignee: Minerals and Chemicals Philipp Corp
•
Filing: 1962-01-10
•
Granted: 1965-11-02
•
Expires: 1982-01-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Glen A Hemstock

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 09:48
CPC Classifications
C; C01; C01B; C01B33/00; C01B33/20; C01B33/22

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 63 words
A METHOD OF TREATING CHRYSOTILE WITH COMPRISES CALCINING CHRYSOTILE AT A TEMPERATURE WITHIN THE RANGE OF 650*C. TO 1100*C. AND FOR A TIME SUFFICIENT TO DESTROY THE CHRYSOTILE CRYSTAL STRUCTURE AND SUBJECTING THE CALCINED CHRYSOTILE TO HYDROTHERMAL TREATMENT UNDER SUPERATMOSPHERIC PRESSURE UNTIL THE WATER OF CRYSTALLIZATION OF SAID CALCINED CHRYSOTILE IS WITHIN THE RANGE OF FROM AB OUT 5.3% TO AB OUT 5.9%.
Claim 2
Independent Claim 63 words
A METHOD OF TREATING CHRYSOTILE WITH COMPRISES CALCINING CHRYSOTILE AT A TEMPERATURE WITHIN THE RANGE OF 650*C. TO 1100*C. AND FOR A TIME SUFFICIENT TO DESTROY THE CHRYSOTILE CRYSTAL STRUCTURE AND SUBJECTING THE CALCINED CHRYSOTILE TO HYDROTHERMAL TREATMENT UNDER SUPERATMOSPHERIC PRESSURE UNTIL THE WATER OF CRYSTALLIZATION OF SAID CALCINED CHRYSOTILE IS WITHIN THE RANGE OF FROM AB OUT 5.3% TO AB OUT 5.9%.

References Cited (Backward Citations)

US2616801A Cited
US2926997A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-11-01 1969-05-03 1969-11-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-11-01 1973-05-03 1973-11-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-11-01 1977-05-03 1977-11-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag