← Back to Patent Explorer
US3205204A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for polymerization of vinyl chloride

Assignee: Wacker Chemie AG
•
Filing: 1961-12-12
•
Granted: 1965-09-07
•
Expires: 1981-12-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Heckmaier Joseph
  • 👤 Bauer Hans

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 09:19
CPC Classifications
C; C08; C08F; C08F2/00; C08F2/04; C08F2/10; C08F14/00; C08F14/02; C08F14/04; C08F14/06; Y; Y10; Y10S; Y10S526/00; Y10S526/909; Y10S526/911

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 123 words
IN THE PROCESS OF PREPARING A POLYMERIZATE OF A VINYL MONOMER SELECTED FROM THE GROUP CONSISTING OF VINYL CHLORIDE AND MIXTURES OF VINYL CHLORIDE WITH UP TO 10% OF A VINYL ESTER OF A LOWER ALKANOIC ACID, IN WATER IN THE PRESENCE OF A FREE-RADICAL, MONOMER-SOLUBLE POLYMERIZATION CATALYST, WATER-SOLUBLE, INORGANIC BUFFER SALTS, AND A WATERSOLUBLE COLLOIDAL SUSPENSION AGENT, BY AGITATING THE MIXTURE AT A TEMPERATURE BETWEEN ABOUT 0*C. AND 80*C. FOR A TIME SUFFICIENT TO EFFECT POLYMERIZATION, THE IMPROVEMENT WHICH COMPRISES UTILIZING AS SAID SUSPENSION AGENT ABOUT 0.01% TO 0.25% BASED ON THE WEIGHT OF THE VINYL MONOMER, OF A WATER-SOLUBLE METHYL CELLULOSE PREPARED BY THE REACTION OF LIQUID METHYL CHLORIDE WITH AN ALKALI METAL CELLULOSE AT A TEMPERATURE BETWEEN 40*C. AND 90*C.
Claim 2
Dependent Claim 123 words
IN THE PROCESS OF PREPARING A POLYMERIZATE OF A VINYL MONOMER SELECTED FROM THE GROUP CONSISTING OF VINYL CHLORIDE AND MIXTURES OF VINYL CHLORIDE WITH UP TO 10% OF A VINYL ESTER OF A LOWER ALKANOIC ACID, IN WATER IN THE PRESENCE OF A FREE-RADICAL, MONOMER-SOLUBLE POLYMERIZATION CATALYST, WATER-SOLUBLE, INORGANIC BUFFER SALTS, AND A WATERSOLUBLE COLLOIDAL SUSPENSION AGENT, BY AGITATING THE MIXTURE AT A TEMPERATURE BETWEEN ABOUT 0*C. AND 80*C. FOR A TIME SUFFICIENT TO EFFECT POLYMERIZATION, THE IMPROVEMENT WHICH COMPRISES UTILIZING AS SAID SUSPENSION AGENT ABOUT 0.01% TO 0.25% BASED ON THE WEIGHT OF THE VINYL MONOMER, OF A WATER-SOLUBLE METHYL CELLULOSE PREPARED BY THE REACTION OF LIQUID METHYL CHLORIDE WITH AN ALKALI METAL CELLULOSE AT A TEMPERATURE BETWEEN 40*C. AND 90*C.

References Cited (Backward Citations)

GB754876A Cited
US2875185A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-09-06 1969-03-08 1969-09-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-09-06 1973-03-08 1973-09-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-09-06 1977-03-08 1977-09-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag