← Back to Patent Explorer
US3203913A Expired / Lapsed US ⏱️ 0.0 years remaining

Cured composition prepared from mixture of polypropylene glycol ether, diisocyanate, aromatic diamine and cellulosic filler

Assignee: Goodyear Tire and Rubber Co
•
Filing: 1962-04-02
•
Granted: 1965-08-31
•
Expires: 1982-04-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Anthony F Finelli

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 08:49
CPC Classifications
C; C08; C08G; C08G18/00; C08G18/06; C08G18/28; C08G18/40; C08G18/48; C08G18/4825; A; A43; A43B; A43B13/00; A43B13/02; A43B13/04; C08G18/08; C08G18/10; C08L; C08L75/00; C08L75/04; C08L75/08

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 156 words
A CURED POLYURETHANE COMPOSITION SUITABLE FOR THE WEARING SURFACE OF A SHOE RESULTING FROM THE REACTION OF A FLUID MIXTURE COMPRISING (1) A POLYPROPYLENE ETHER GLYCOL CONTAINING LESS THAN 10 MOLE PERCENT OF ETHYLENE ETHER AND HAVING A MOLECULAR WEIGHT OF 800 TO 1600; (2) AN ORGANO DIISOCYANATE SELECTED FROM THE CLASS CONSISTING OF DIPHENYL METHANE-4,4''-DIISOCYANATE AND THE TOLYLENE DIISOCYAMATES; (3) A CHLORINATED AROMATIC DIAMINE; (4) A CELLULOSIC FLOUR SELECTED FROM THE CLASS CONSISTING OF WOOD FLOURS AND NUT SHELL FLOURS; (5) SAID DIAMINE TO EXCESS DIISOCYANATE RATIO BEING FROM 0.5 TO 1.0; (6) SAID DIISOCYANATE BEING PRESENT IN 1.7 TO 2.5 MOLS PER MOL OF POLYPROPYLENE ETHER GLYCOL; AND (7) SAID CELLULOSIC FLOURS BEING PRESENT IN AN AMOUNT RANGING FROM 60 TO 100 PARTS BY WEIGHT PER HUNDRED PARTS OF POLYPROYLENE ETHER GLYCOL AND BEING CHARACTERIZED BY THE ABILITY TO FORM A POURABLE MIXTURE WHEN MIXED WITH SAID POLYPROPYLENE ETHER GLYCOL IN THE ABOVE AMOUNTS.
Claim 2
Dependent Claim 156 words
A CURED POLYURETHANE COMPOSITION SUITABLE FOR THE WEARING SURFACE OF A SHOE RESULTING FROM THE REACTION OF A FLUID MIXTURE COMPRISING (1) A POLYPROPYLENE ETHER GLYCOL CONTAINING LESS THAN 10 MOLE PERCENT OF ETHYLENE ETHER AND HAVING A MOLECULAR WEIGHT OF 800 TO 1600; (2) AN ORGANO DIISOCYANATE SELECTED FROM THE CLASS CONSISTING OF DIPHENYL METHANE-4,4''-DIISOCYANATE AND THE TOLYLENE DIISOCYAMATES; (3) A CHLORINATED AROMATIC DIAMINE; (4) A CELLULOSIC FLOUR SELECTED FROM THE CLASS CONSISTING OF WOOD FLOURS AND NUT SHELL FLOURS; (5) SAID DIAMINE TO EXCESS DIISOCYANATE RATIO BEING FROM 0.5 TO 1.0; (6) SAID DIISOCYANATE BEING PRESENT IN 1.7 TO 2.5 MOLS PER MOL OF POLYPROPYLENE ETHER GLYCOL; AND (7) SAID CELLULOSIC FLOURS BEING PRESENT IN AN AMOUNT RANGING FROM 60 TO 100 PARTS BY WEIGHT PER HUNDRED PARTS OF POLYPROYLENE ETHER GLYCOL AND BEING CHARACTERIZED BY THE ABILITY TO FORM A POURABLE MIXTURE WHEN MIXED WITH SAID POLYPROPYLENE ETHER GLYCOL IN THE ABOVE AMOUNTS.

References Cited (Backward Citations)

US2968575A Cited
US2983702A Cited
US3022257A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-08-30 1969-03-01 1969-08-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-08-30 1973-03-01 1973-08-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-08-30 1977-03-01 1977-08-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag