Silver halide sensitized lithographic printing plate
Assignee: Eastman Kodak Co
•
Filing: 1959-12-21
•
Granted: 1964-08-25
•
Expires: 1979-12-21
Abstract
No abstract record available.
Inventors
- 👤 Edward C Yackel
- 👤 Thomas I Abbott
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-01 14:45
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/06
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
122 words
A LITHOGRAPHIC PRINTING PROCESS WHICH COMPRISES (A) EXPOSING TO A SUBJECT A PHOTOGRAPHIC ELEMENT COMPRISING A SUPPORT HAVING THEREON A GELATIN LAYER CONTAINING A SUFFICIENT AMOUNT OF A POLYHYDROXYBENZENE SILVER HALIDE DEVELOPING AGENT TO DEVELOP THE EXPOSED SILVER HALIDE IN THE LIGHT-SENSITIVE LAYER ABOVE IT, SAID AGENT SELECTED FROM THE CLASS CONSISTING OF HALOGEN SUBSTITUTED, PHENYL SUBSTITUTED, AND 2-6 CARBON ATOMS CONTAINING ALKYL SUBSTITUTED POLYHYDROXYBENZENE DEVELOPING AGENTS, THE OXIDATION PRODUCT OF WHICH RENDERS GELATIN OLEOPHILIC AND OVER SAID GELATIN LAYER AN UNFOGGED GELATINO-SILVER HALIDE EMULSION LAYER UNIFORMLY HARDENED WITH A HARDENER, SUCH THAT THE GELATIN HAS A HARDNESS EQUIVALENT TO THAT OF A GELATIN LAYER HARDENED WITH ABOUT 2 GRAMS TO ABOUT 15 GRAMS OF DRY FORMALDEHYDE PER POUND OF GELATIN, AND
Claim 2
Dependent Claim
122 words
A LITHOGRAPHIC PRINTING PROCESS WHICH COMPRISES (A) EXPOSING TO A SUBJECT A PHOTOGRAPHIC ELEMENT COMPRISING A SUPPORT HAVING THEREON A GELATIN LAYER CONTAINING A SUFFICIENT AMOUNT OF A POLYHYDROXYBENZENE SILVER HALIDE DEVELOPING AGENT TO DEVELOP THE EXPOSED SILVER HALIDE IN THE LIGHT-SENSITIVE LAYER ABOVE IT, SAID AGENT SELECTED FROM THE CLASS CONSISTING OF HALOGEN SUBSTITUTED, PHENYL SUBSTITUTED, AND 2-6 CARBON ATOMS CONTAINING ALKYL SUBSTITUTED POLYHYDROXYBENZENE DEVELOPING AGENTS, THE OXIDATION PRODUCT OF WHICH RENDERS GELATIN OLEOPHILIC AND OVER SAID GELATIN LAYER AN UNFOGGED GELATINO-SILVER HALIDE EMULSION LAYER UNIFORMLY HARDENED WITH A HARDENER, SUCH THAT THE GELATIN HAS A HARDNESS EQUIVALENT TO THAT OF A GELATIN LAYER HARDENED WITH ABOUT 2 GRAMS TO ABOUT 15 GRAMS OF DRY FORMALDEHYDE PER POUND OF GELATIN, AND
References Cited (Backward Citations)
US1742710A
Cited
US1961927A
Cited
US2372873A
Cited
US2444205A
Cited
US2661293A
Cited
US2565376A
Cited
US2592368A
Cited
US2593912A
Cited
US2685510A
Cited
US2725298A
Cited
US2704712A
Cited
US2937945A
Cited
US3038804A
Cited
US3039869A
Cited
US2996382A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1967-08-25 | 1968-02-24 | 1968-08-25 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1971-08-25 | 1972-02-24 | 1972-08-25 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1975-08-25 | 1976-02-24 | 1976-08-25 | $7700.00 | Window Closed / Lapsed |