US3136676A Expired / Lapsed US ⏱️ 0.0 years remaining

Metallized plastic extrusion products and method of making same

Assignee: Anchor Plastics Co Inc
•
Filing: 1957-02-20
•
Granted: 1964-06-09
•
Expires: 1977-02-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Fisch Hilde
  • 👤 Guggenheimer William

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 20:07
CPC Classifications
B; B29; B29C; B29C70/00; B29C70/58; B29C48/00; B29C48/03; B29C48/05; B29C48/07; B29C48/08; B29C48/15; B29C48/154; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49123; Y10T29/49826; Y10T29/49888

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 114 words
IN THE PROCESS OF PREPARING EXTRUDED THERMOPLASTIC PRODUCTS WITH AT LEAST ONE VISIBLE REGION THEREOF HAVING A METALLIC APPEARANCE, THE STEPS COMPRISING PROVIDING A METAL FOIL HAVING A THIN, FILM-LIKE COATING OF A TRANSPARENT THERMOPLASTIC LACQUER OF THE GROUP CONSISTING OF CELLULOSE NITRATE, CELLULOSE BUTYRATE, ETHYL CELLULOSE, AND POLYVINYL ACETATE-POLYVINYL CHLORIDE LACQUERS ON AT LEAST ONE SURFACE THEREOF, EXTRUDING A TRANSPARENT THERMOPLASTIC MATERIAL ABOUT THE LACQUER-COATED FOIL WHILE FEEDING THE FOIL IN UNISON WITH THE THERMOPLASTIC MATERIAL WITH THE SURFACE OF THE FOIL CONTAINING THE LACQUER COATING CONTACTING THE INTERIOR SURFACE OF THE EXTRUDED MATERIAL WHEREBY THE LAQUER-COATING OF THE FOIL ADHESIVELY FIXES THE POSITION OF THE LATTER WITH RESPECT TO THE EXTRUDED MATERIAL.
Claim 2
Dependent Claim 114 words
IN THE PROCESS OF PREPARING EXTRUDED THERMOPLASTIC PRODUCTS WITH AT LEAST ONE VISIBLE REGION THEREOF HAVING A METALLIC APPEARANCE, THE STEPS COMPRISING PROVIDING A METAL FOIL HAVING A THIN, FILM-LIKE COATING OF A TRANSPARENT THERMOPLASTIC LACQUER OF THE GROUP CONSISTING OF CELLULOSE NITRATE, CELLULOSE BUTYRATE, ETHYL CELLULOSE, AND POLYVINYL ACETATE-POLYVINYL CHLORIDE LACQUERS ON AT LEAST ONE SURFACE THEREOF, EXTRUDING A TRANSPARENT THERMOPLASTIC MATERIAL ABOUT THE LACQUER-COATED FOIL WHILE FEEDING THE FOIL IN UNISON WITH THE THERMOPLASTIC MATERIAL WITH THE SURFACE OF THE FOIL CONTAINING THE LACQUER COATING CONTACTING THE INTERIOR SURFACE OF THE EXTRUDED MATERIAL WHEREBY THE LAQUER-COATING OF THE FOIL ADHESIVELY FIXES THE POSITION OF THE LATTER WITH RESPECT TO THE EXTRUDED MATERIAL.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1967-06-09 1967-12-09 1968-06-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1971-06-09 1971-12-09 1972-06-09 $3760.00 Window Closed / Lapsed