Establishment of ph value of a phosphoric acid solution by its reaction with iron prior to its use to treat ferrous surfaces

Assignee: Individual
•
Filing: 1961-03-20
•
Granted: 1963-09-03
•
Expires: 1981-03-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Duchange Guillaume

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 23:49
CPC Classifications
C; C23; C23C; C23C22/00; C23C22/05; C23C22/06; C23C22/24; C23C22/33

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 135 words
AN ANTI-CORROSION TREATMENT OF FERROUS SURFACES, CONSISTING IN DISSOLVING IN 760 PARTS BY VOLUME OF WATER 12 PARTS BY WEIGHT OF SALT SELECTED FROM THE GROUP CONSISTING OF SODIUM BICHROMATE AND POTASSIUM BICHROMATE, 6 PARTS BY WEIGHT OF A SLAT SELECTED FROM THE GROUP CONSISTING OF TRISODIUM PHOSPHATE, DISODIUM PHSOSPHATE AND MONOSODIUM PHOSPHATE, 240 PARYS BY VOLUME OF 58*B. ORTHOPHOSPHORIC ACID, ADDING TO THE RESULTING SOLUTION 7.60 PARTS BY WEIGHT OF A ZINC COMPOUND SELECTED FROM THE GROUP CONSISTING OF ZINC OXIDE AND ZINC SULFATE, REACTING THE MIXTURE SO FORMED WITH IRON BY IMMERGING THEREIN AN IRON PIECE UNTIL SAID MIXTURE SHOWS A GREEN COLOR AND HAS A PH VALUE OF 2.5, ADDING 10 TO 12 PARTS BY WEIGHT OF A CELLULOSE ESTER TO THE GREEN-COLORED MIXTURE, AND APPLYING THE SAME TO SAID FERROUS SURFACES.
Claim 2
Dependent Claim 135 words
AN ANTI-CORROSION TREATMENT OF FERROUS SURFACES, CONSISTING IN DISSOLVING IN 760 PARTS BY VOLUME OF WATER 12 PARTS BY WEIGHT OF SALT SELECTED FROM THE GROUP CONSISTING OF SODIUM BICHROMATE AND POTASSIUM BICHROMATE, 6 PARTS BY WEIGHT OF A SLAT SELECTED FROM THE GROUP CONSISTING OF TRISODIUM PHOSPHATE, DISODIUM PHSOSPHATE AND MONOSODIUM PHOSPHATE, 240 PARYS BY VOLUME OF 58*B. ORTHOPHOSPHORIC ACID, ADDING TO THE RESULTING SOLUTION 7.60 PARTS BY WEIGHT OF A ZINC COMPOUND SELECTED FROM THE GROUP CONSISTING OF ZINC OXIDE AND ZINC SULFATE, REACTING THE MIXTURE SO FORMED WITH IRON BY IMMERGING THEREIN AN IRON PIECE UNTIL SAID MIXTURE SHOWS A GREEN COLOR AND HAS A PH VALUE OF 2.5, ADDING 10 TO 12 PARTS BY WEIGHT OF A CELLULOSE ESTER TO THE GREEN-COLORED MIXTURE, AND APPLYING THE SAME TO SAID FERROUS SURFACES.

References Cited (Backward Citations)

US2516685A Cited
US2800422A Cited
US2711391A Cited
US2900222A Cited
US2798016A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-09-02 1967-03-04 1967-09-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-09-02 1971-03-04 1971-09-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-09-02 1975-03-04 1975-09-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag