← Back to Patent Explorer
US3080207A Expired / Lapsed US ⏱️ 0.0 years remaining

Preparation of polyvinyl alcohol bodies having improved knot strength

Assignee: Kurashiki Rayon Co Ltd
•
Filing: 1959-03-26
•
Granted: 1963-03-05
•
Expires: 1979-03-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Tanabe Kenichi
  • 👤 Ohno Yasuji

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-22 19:17
CPC Classifications
D; D06; D06M; D06M13/00; D06M13/10; D06M13/12; D06M13/123; Y; Y10; Y10S; Y10S8/00; Y10S8/10

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 162 words
A PROCESS FOR IMPROVING THE KNOT STRENGTH AN ELASTIC RECOVERY OF POLYVINYL ALCOHOL FIBRES WHICH CONSISTS ESSENTIALLY OF RAPIDLY ACETALIZING THE SAID FIBERS BY REACTION WITH AN ALDEHYDE CONSISTING ESSENTIALLY OF AN ALIPHATIC DIALDEHYDE SELECTED FROM THE GROUP CONSISTING OF SUCCINIC DIALEHYDE AND GLUTARIC DIALDEHYDE, IN AN AQUEOUS SOLUTION CONTAINING A HIGH CONCENTRATION OF A CATALYST SELECTED FROM THE GROUP CONSISTING OF SULFURIC ACID, PHOSPHORIC ACID, AND HYDROCHLORIC ACID, THE CONCENTRATION OF SULFURIC ACID IN SAID AQUEOUS SOLUTION BEING AT LEAST 8% BY WEIGHT WHEN SULFURIC ACID IS EMPLOYED, THE CONCENTRATION OF HYDROCHLORIC ACID IN SAID SOLUTION BEING AT LEAST 2% BY WEIGHT WHEN HYDROCHLORIC ACID IS EMPLOYED, AND THE CONCENTRATION OF PHOSPHORIC ACID IN SAID SOLUTION BEING AT LEAST 10% BY WEIGHT WHEN PHOSPHORIC ACID IS EMPLOYED, THE ACETALIZATION BEING CARRIED OUT UNTIL THE WEIGHT OF THE FIBERS IS INCREASED DUE TO THE ACETALIZATION BY ABOUT 1 TO 20%, SAID ACETALIZATION BEING CARRIED OUT AT A TEMPETATURE OF 40 TO 70*C.
Claim 2
Dependent Claim 162 words
A PROCESS FOR IMPROVING THE KNOT STRENGTH AN ELASTIC RECOVERY OF POLYVINYL ALCOHOL FIBRES WHICH CONSISTS ESSENTIALLY OF RAPIDLY ACETALIZING THE SAID FIBERS BY REACTION WITH AN ALDEHYDE CONSISTING ESSENTIALLY OF AN ALIPHATIC DIALDEHYDE SELECTED FROM THE GROUP CONSISTING OF SUCCINIC DIALEHYDE AND GLUTARIC DIALDEHYDE, IN AN AQUEOUS SOLUTION CONTAINING A HIGH CONCENTRATION OF A CATALYST SELECTED FROM THE GROUP CONSISTING OF SULFURIC ACID, PHOSPHORIC ACID, AND HYDROCHLORIC ACID, THE CONCENTRATION OF SULFURIC ACID IN SAID AQUEOUS SOLUTION BEING AT LEAST 8% BY WEIGHT WHEN SULFURIC ACID IS EMPLOYED, THE CONCENTRATION OF HYDROCHLORIC ACID IN SAID SOLUTION BEING AT LEAST 2% BY WEIGHT WHEN HYDROCHLORIC ACID IS EMPLOYED, AND THE CONCENTRATION OF PHOSPHORIC ACID IN SAID SOLUTION BEING AT LEAST 10% BY WEIGHT WHEN PHOSPHORIC ACID IS EMPLOYED, THE ACETALIZATION BEING CARRIED OUT UNTIL THE WEIGHT OF THE FIBERS IS INCREASED DUE TO THE ACETALIZATION BY ABOUT 1 TO 20%, SAID ACETALIZATION BEING CARRIED OUT AT A TEMPETATURE OF 40 TO 70*C.

References Cited (Backward Citations)

US2636803A Cited
US2749208A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-03-04 1966-09-03 1967-03-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-03-04 1970-09-03 1971-03-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-03-04 1974-09-03 1975-03-05 $7700.00 Window Closed / Lapsed