US3076248A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for the production of calcined phosphate agglomerates

Assignee: FMC Corp
•
Filing: 1960-11-17
•
Granted: 1963-02-05
•
Expires: 1980-11-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Wendell L Darrow
  • 👤 Joseph W Kass

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 16:35
CPC Classifications
B; B01; B01J; B01J2/00; B01J2/26; C; C01; C01B; C01B25/00; C01B25/01; Y; Y10; Y10S; Y10S425/00; Y10S425/101

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 163 words
THE METHOD OF PRODUCING A PHOSPHATE AGGLOMERATE HAVING A HIGH STRUCTURAL STRENGTH WHICH COMPRISES PLACING A CRUSHED PHOSPHATE LUMP HAVING A PARTICLE SIZE OF ABOUT 1/4 TO ABOUT 3 INCHES IN DIAMETER ON A NON-AGITATED PERFORATE CARRIER TO FORM AN UNDERHEARTH LAYER, PLACING AN OVERLAY OF AGGLOMERATE PHOSPHATE FEED ON SAID UNDERHEARTH LAYER TO FORM A FEED BED, SAID AGGLOMERATE PHOSPHATE FEED BEING FORMED BY THE AGGLOMERATION OF CRUSHED PHOSPHATE ORE CONTAINING MINOR AMOUNTS OF SHALE OIL AND CAPABLE OF PASSING THROUGH A 6 MM. SCREEN, MAINTAINING SAID UNDERHEARTH LAYER IN PROPORTIONS OF AT LEAST ABOUT 16% OF THE TOTAL FEED BED DEPTH, PASSING SAID FEED BED THROUGH A CALCINING ZONE, PASSING A HEATED GAS THROUGH SAID FEED BED IN SAID CALCINING ZONE AND HEATING SAID AGGLOMERATES TO TEMPERATURES BETWEEN ABOUT 2250 TO 2500*F., MAINTAINING SAID FEED BED IN THE CALCINING ZONE FOR FROM ABOUT 15 TO 25 MINUTES, PASSING THE RESULTING CALCINING PHOSPHATE INTO A COOLING ZONE AND RECOVERING THE CALCINED PRODUCT.
Claim 2
Independent Claim 163 words
THE METHOD OF PRODUCING A PHOSPHATE AGGLOMERATE HAVING A HIGH STRUCTURAL STRENGTH WHICH COMPRISES PLACING A CRUSHED PHOSPHATE LUMP HAVING A PARTICLE SIZE OF ABOUT 1/4 TO ABOUT 3 INCHES IN DIAMETER ON A NON-AGITATED PERFORATE CARRIER TO FORM AN UNDERHEARTH LAYER, PLACING AN OVERLAY OF AGGLOMERATE PHOSPHATE FEED ON SAID UNDERHEARTH LAYER TO FORM A FEED BED, SAID AGGLOMERATE PHOSPHATE FEED BEING FORMED BY THE AGGLOMERATION OF CRUSHED PHOSPHATE ORE CONTAINING MINOR AMOUNTS OF SHALE OIL AND CAPABLE OF PASSING THROUGH A 6 MM. SCREEN, MAINTAINING SAID UNDERHEARTH LAYER IN PROPORTIONS OF AT LEAST ABOUT 16% OF THE TOTAL FEED BED DEPTH, PASSING SAID FEED BED THROUGH A CALCINING ZONE, PASSING A HEATED GAS THROUGH SAID FEED BED IN SAID CALCINING ZONE AND HEATING SAID AGGLOMERATES TO TEMPERATURES BETWEEN ABOUT 2250 TO 2500*F., MAINTAINING SAID FEED BED IN THE CALCINING ZONE FOR FROM ABOUT 15 TO 25 MINUTES, PASSING THE RESULTING CALCINING PHOSPHATE INTO A COOLING ZONE AND RECOVERING THE CALCINED PRODUCT.

References Cited (Backward Citations)

US2174066A Cited
US2900179A Cited
US2776828A Cited
US2945688A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-02-04 1966-08-06 1967-02-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-02-04 1970-08-06 1971-02-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-02-04 1974-08-06 1975-02-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag