← Back to Patent Explorer
US3073729A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for producing predetermined secondary recrystallization textures in metals

Assignee: Vacuumschmelze GmbH and Co KG
•
Filing: 1960-06-01
•
Granted: 1963-01-15
•
Expires: 1980-06-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Hans G Baer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 21:06
CPC Classifications
C; C21; C21D; C21D8/00; C21D8/12; C21D1/00; C21D1/78; C21D2281/00; C21D2281/01

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 174 words
IN THE PROCESS OF CAUSING A PREDETERMINED SECONDARY RECRYSTALLIZATION TEXTURE IN A FIRST SHEET OF A METAL WHICH CAN ATTAIN SUCH SECONDARY RECRYSTALLIZATION TEXTURE BUT HAS NOT BEEN PREVIOUSLY SUBJECTED TO SECONDARY RECRYSTALLIZATION, THE STEPS COMPRISING DISPOSING SAID FIRST METAL SHEET IN INTIMATE CONTACT OF SELECTED PORTION OF ITS SURFACE WITH A SURFACE OF A STIMULATING SHEET OF A METAL WHICH AT THE ANNEALING TEMPERATURES NECESSARY TO EFFECT SECONDARY RECRYSTALLIZATION HAS THE SAME CRYSTAL STRUCTURE AS THE SAID FIRST METAL SHEET AND HAVING A CRYSTAL STRUCTURE THAT WILL YIELD THE PREDETERMINED SECONDARY CRYSTAL STRUCTURE DURING SECONDARY RECRYSTALLIZATION, THE CONTACTING SURFACES OF THE SHEETS BEING CLEAN, THE STIMULATING SHEET READILY ATTAINING A GIVEN SECONDARY RECRYSTALLIZATION TEXTURE AT THE ANNEALING TEMPERATURE, AND HEATING THE ASSEMBLED SHEETS TO ANNEALING TEMPERATURES, AND TEMPERATURE, THE CLEANLINESS, AND THE INTIMATE CONTACT BETWEEN THE SURFACES PRODUCING AT LEAST A PARTIAL WELDING OF THE SURFACES, AND CONTINUING THE ANNEALING UNTIL SECONDARY RECRYSTALLIZATION GRAIN GROWTH OF THE STIMULATING SHEET HAS OCCURRED AND HAS INDUCED A CORRESPONDING SECONDARY RECRYSTALLIZATION TEXTURE IN THE FIRST SHEET.
Claim 2
Dependent Claim 174 words
IN THE PROCESS OF CAUSING A PREDETERMINED SECONDARY RECRYSTALLIZATION TEXTURE IN A FIRST SHEET OF A METAL WHICH CAN ATTAIN SUCH SECONDARY RECRYSTALLIZATION TEXTURE BUT HAS NOT BEEN PREVIOUSLY SUBJECTED TO SECONDARY RECRYSTALLIZATION, THE STEPS COMPRISING DISPOSING SAID FIRST METAL SHEET IN INTIMATE CONTACT OF SELECTED PORTION OF ITS SURFACE WITH A SURFACE OF A STIMULATING SHEET OF A METAL WHICH AT THE ANNEALING TEMPERATURES NECESSARY TO EFFECT SECONDARY RECRYSTALLIZATION HAS THE SAME CRYSTAL STRUCTURE AS THE SAID FIRST METAL SHEET AND HAVING A CRYSTAL STRUCTURE THAT WILL YIELD THE PREDETERMINED SECONDARY CRYSTAL STRUCTURE DURING SECONDARY RECRYSTALLIZATION, THE CONTACTING SURFACES OF THE SHEETS BEING CLEAN, THE STIMULATING SHEET READILY ATTAINING A GIVEN SECONDARY RECRYSTALLIZATION TEXTURE AT THE ANNEALING TEMPERATURE, AND HEATING THE ASSEMBLED SHEETS TO ANNEALING TEMPERATURES, AND TEMPERATURE, THE CLEANLINESS, AND THE INTIMATE CONTACT BETWEEN THE SURFACES PRODUCING AT LEAST A PARTIAL WELDING OF THE SURFACES, AND CONTINUING THE ANNEALING UNTIL SECONDARY RECRYSTALLIZATION GRAIN GROWTH OF THE STIMULATING SHEET HAS OCCURRED AND HAS INDUCED A CORRESPONDING SECONDARY RECRYSTALLIZATION TEXTURE IN THE FIRST SHEET.

References Cited (Backward Citations)

US2165027A Cited
US2753623A Cited
US2700006A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-01-14 1966-07-16 1967-01-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-01-14 1970-07-16 1971-01-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-01-14 1974-07-16 1975-01-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag