← Back to Patent Explorer
US3066115A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for the polymerization of ethylenically unsaturated monomers with a diphenylethane accelerator

Assignee: BX Plastics Ltd
•
Filing: 1958-11-28
•
Granted: 1962-11-27
•
Expires: 1978-11-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Smith Robert Roy
  • 👤 Mann Dennis Charles Macmillan
  • 👤 Logie Gordon Robertson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 12:30
CPC Classifications
C; C08; C08F; C08F18/00; C08F18/02; C08F18/04; C08F18/08; C08F12/00; C08F12/02; C08F12/04

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 133 words
A PROCESS FOR THE POLYMERISATION IN MASS OF UNSATURATED COMPOUNDS CONTAINING ETHYLENIC LINKAGES SELECTED FROM THE GROUP CONSISTING OF STYRENE, ORTHO-, META- AMD PARA-VINYL TOLUENES AND DIALLYL PHTHALATE MONOMERS, WHICH COMPRISES THE STEP OF PARTIALLY POLYMERISING THE SAID UNSATURATED COMPOUND IN A FIRST STAGE BY HEATING TO A TEMPERATURE OF AT MOST 125*C. UNTIL THE POLYMERISABLE COMPOUND HAS BEEN CONVERTED TO AN EXTENT OF AT LEAST 30%, ANY POLYMERISATION INITIATOR USED IN THIS STAGE BEING ONE THAT DISSOCIATES TO GIVE FREE RADICALS, AND THEREAFTER FURTHER POLYMERISING THE COMPOUND BY HEATING IT IN A FINAL STAGE TO A TEMPERATURE WITHIN THE RANGE OF 150 TO 250*C. WHILE CATALYTICALLY ACCELERATING THE RATE OF POLYMERISATION TO A SIGNIFICANT EXTENT BY THE INCORPORATION OF AT LEAST 0.001% BY WEIGHT OF A DIPHENYLETHANE COMPOUND OF THE GENERAL FORMULA
Claim 2
Dependent Claim 133 words
A PROCESS FOR THE POLYMERISATION IN MASS OF UNSATURATED COMPOUNDS CONTAINING ETHYLENIC LINKAGES SELECTED FROM THE GROUP CONSISTING OF STYRENE, ORTHO-, META- AMD PARA-VINYL TOLUENES AND DIALLYL PHTHALATE MONOMERS, WHICH COMPRISES THE STEP OF PARTIALLY POLYMERISING THE SAID UNSATURATED COMPOUND IN A FIRST STAGE BY HEATING TO A TEMPERATURE OF AT MOST 125*C. UNTIL THE POLYMERISABLE COMPOUND HAS BEEN CONVERTED TO AN EXTENT OF AT LEAST 30%, ANY POLYMERISATION INITIATOR USED IN THIS STAGE BEING ONE THAT DISSOCIATES TO GIVE FREE RADICALS, AND THEREAFTER FURTHER POLYMERISING THE COMPOUND BY HEATING IT IN A FINAL STAGE TO A TEMPERATURE WITHIN THE RANGE OF 150 TO 250*C. WHILE CATALYTICALLY ACCELERATING THE RATE OF POLYMERISATION TO A SIGNIFICANT EXTENT BY THE INCORPORATION OF AT LEAST 0.001% BY WEIGHT OF A DIPHENYLETHANE COMPOUND OF THE GENERAL FORMULA

References Cited (Backward Citations)

US2902464A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1965-11-26 1966-05-28 1966-11-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1969-11-26 1970-05-28 1970-11-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1973-11-26 1974-05-28 1974-11-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag