Method of constructing nickel-cadmium cells

Assignee: Union Carbide Corp
•
Filing: 1959-08-10
•
Granted: 1961-09-26
•
Expires: 1979-08-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 John L S Daley

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 14:21
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/24; H01M10/28; H01M10/283; H01M10/34; H01M10/42; H01M10/52; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y02P; Y02P70/00; Y02P70/50; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49108

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 136 words
IN A METHOD OF ASSEMBLING A SEALED NICKEL CADMIUM SECONDARY CELL WHICH COMPRISES AS COMPONENTS A CONTAINER, A COVER FOR SAID CONTAINER, A SEAL GASKET THEREBETWEEN, A NEGATIVE CADMIUM ELECTRODE, A POSITIVE NICKEL ELECTRODE, A SEPARATOR BETWEEN SAID POSITIVE ELECTRODE AND SAID NEGATIVE ELECTRODE AND AN ALKALINE ELECTROLYTE THROUGHOUT, THE IMPROVEMENT WHICH COMPRISES DIMENSIONING SAID COMPONENTS TO FIT LOOSELY WITHIN SAID CONTAINER UPON ASSEMBLING SAID CELL IN ORDER THAT SAID POSITIVE ELECTRODE IS FREE TO SWELL TO APPROXIMATELY THE POINT OF OPTIMUM ELECTRONIC CONDUCTIVITY AND ELECTROLYTIC EFFICIENCY TO ACHIEVE MAXIMUM OUTPUT UPON THE INITIAL CYCLING OF SAID CELL SUBSEQUENT TO THE SEALING OF SAID CELL, SAID DIMENSIONS OF SAID COMPONENTS BEING SUCH THAT SAID SWELLING RESULTS IN TIGHT INTRA-CELL CONTACTS WHEN FURTHER SWELLING OF SAID POSITIVE ELECTRODE IS CONSTRAINED BY SAID NEGATIVE ELECTRODE AND SAID CONTAINER.
Claim 2
Dependent Claim 136 words
IN A METHOD OF ASSEMBLING A SEALED NICKEL CADMIUM SECONDARY CELL WHICH COMPRISES AS COMPONENTS A CONTAINER, A COVER FOR SAID CONTAINER, A SEAL GASKET THEREBETWEEN, A NEGATIVE CADMIUM ELECTRODE, A POSITIVE NICKEL ELECTRODE, A SEPARATOR BETWEEN SAID POSITIVE ELECTRODE AND SAID NEGATIVE ELECTRODE AND AN ALKALINE ELECTROLYTE THROUGHOUT, THE IMPROVEMENT WHICH COMPRISES DIMENSIONING SAID COMPONENTS TO FIT LOOSELY WITHIN SAID CONTAINER UPON ASSEMBLING SAID CELL IN ORDER THAT SAID POSITIVE ELECTRODE IS FREE TO SWELL TO APPROXIMATELY THE POINT OF OPTIMUM ELECTRONIC CONDUCTIVITY AND ELECTROLYTIC EFFICIENCY TO ACHIEVE MAXIMUM OUTPUT UPON THE INITIAL CYCLING OF SAID CELL SUBSEQUENT TO THE SEALING OF SAID CELL, SAID DIMENSIONS OF SAID COMPONENTS BEING SUCH THAT SAID SWELLING RESULTS IN TIGHT INTRA-CELL CONTACTS WHEN FURTHER SWELLING OF SAID POSITIVE ELECTRODE IS CONSTRAINED BY SAID NEGATIVE ELECTRODE AND SAID CONTAINER.

References Cited (Backward Citations)

US2675418A Cited
US2696515A Cited
US2708212A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1964-09-25 1965-03-27 1965-09-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1968-09-25 1969-03-27 1969-09-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1972-09-25 1973-03-27 1973-09-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag