Method for producing improved diamond crystals
Assignee: General Electric Co
•
Filing: 1958-12-29
•
Granted: 1961-07-18
•
Expires: 1978-12-29
Abstract
No abstract record available.
Inventors
- 👤 Harold P Bovenkerk
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 09:31
CPC Classifications
B; B01; B01J; B01J3/00; B01J3/06; B01J3/065; B01J3/062; C; C01; C01B; C01B32/00; C01B32/25; C01B32/26; B01J2203/00; B01J2203/06; B01J2203/0605; B01J2203/0625; B01J2203/065; B01J2203/0655; B01J2203/0675; B01J2203/068; Y; Y10; Y10S; Y10S425/00; Y10S425/026
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
123 words
IN THE SYNTHESIS OF DIAMOND IN A REACTION CHAMBER IN A HIGH PRESSURE HIGH TEMPERATURE APPARATUS WHICH INCLUDES SUBJECTING A COMBINATION OF A NON-DIAMOND FORM OF CARBON AND A DIAMOND CATALYTIC MATERIAL TO SUFFICIENTLY HIGH PRESSURES AND HIGH TEMPERATURES TO OBTAIN A TRANSITION FROM THE NON-DIAMOND FORM OF CARBON TO DIAMOND, THE PROCESS COMPRISING POSITIONING A PLURALITY OF LAMINA OF NON-DIAMOND CARBON IN SAID REACTION CHAMBER, POSITIONING A PLURALITY OF DIAMOND CATALYTIC MATERIAL LAMINA IN SAID REACTION CHAMBER, ARRANGING SAID CATALYST AND SAID CARBON LAMINA IN ALTERNATE LAMINAR RELATIONSHIP, SUBJECTING SAID COMBINATION OF NON-DIAMOND CARBON AND DIAMOND CATALYTIC MATERIAL TO A COMBINED PRESSURE AND TEMPERATURE IN THE REACTION CHAMBER SUFFICIENT TO CAUSE DIAMOND GROWTH FROM SAID NON-DIAMOND CARBON, AND RECOVERING THE DIAMONDS FORMED.
Claim 2
Dependent Claim
123 words
IN THE SYNTHESIS OF DIAMOND IN A REACTION CHAMBER IN A HIGH PRESSURE HIGH TEMPERATURE APPARATUS WHICH INCLUDES SUBJECTING A COMBINATION OF A NON-DIAMOND FORM OF CARBON AND A DIAMOND CATALYTIC MATERIAL TO SUFFICIENTLY HIGH PRESSURES AND HIGH TEMPERATURES TO OBTAIN A TRANSITION FROM THE NON-DIAMOND FORM OF CARBON TO DIAMOND, THE PROCESS COMPRISING POSITIONING A PLURALITY OF LAMINA OF NON-DIAMOND CARBON IN SAID REACTION CHAMBER, POSITIONING A PLURALITY OF DIAMOND CATALYTIC MATERIAL LAMINA IN SAID REACTION CHAMBER, ARRANGING SAID CATALYST AND SAID CARBON LAMINA IN ALTERNATE LAMINAR RELATIONSHIP, SUBJECTING SAID COMBINATION OF NON-DIAMOND CARBON AND DIAMOND CATALYTIC MATERIAL TO A COMBINED PRESSURE AND TEMPERATURE IN THE REACTION CHAMBER SUFFICIENT TO CAUSE DIAMOND GROWTH FROM SAID NON-DIAMOND CARBON, AND RECOVERING THE DIAMONDS FORMED.
References Cited (Backward Citations)
US411017A
Cited
US682249A
Cited
US1637291A
Cited
US2084002A
Cited
US2149596A
Cited
US2554499A
Cited
US2547521A
Cited
US2814552A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1964-07-17 | 1965-01-16 | 1965-07-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1968-07-17 | 1969-01-16 | 1969-07-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1972-07-17 | 1973-01-16 | 1973-07-18 | $7700.00 | Window Closed / Lapsed |