Patent US4468539A successfully refreshed from Google Patents.
← Back to Patent Explorer
US2990291A Expired / Lapsed US ⏱️ 0.0 years remaining

Process of preparing pigment delustered cellulose acetate yarn

Assignee: EIDP Inc
•
Filing: 1960-06-22
•
Granted: 1961-06-27
•
Expires: 1980-06-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Bartholomay Henry William

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 19:43
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/20; C08J3/22; C08J3/226; D; D01; D01D; D01D1/00; D01D1/06; D01D1/065; D01F; D01F1/00; D01F1/02; D01F1/04; D01F2/00; D01F2/24; D01F2/28; C08J2333/00; C08J2333/18; C08J2333/20; C08J2433/00

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 166 words
IN THE PROCESS OF DISPERSING HARD, WHITE, INORGANIC PIGMENT IN CELLULOSE ACETATE SPRINNING SOLUTION AND SPINNING THE SOLUTION TO FORM DELUSTERED CELLULOSE ACETATE YARN, THE IMPROVEMENT FOR REDUCING THE ABRASIVENESS OF THE RESULTING YARN WHICH COMPRISES AND GRINDING A SLURRY OF THE INORGANIC PIGMENT IN AN ACETONE SOLUTION OF CELLULOSE ACETATE, CONTAINING 10-40 PARTS BY WEIGHT OF PIGMENT AND 2-6 PARTS OF CELLULOSE ACETATE PER 100 PARTS OF SLURRY, BY HIGH SPEED AGITATION WITH AN AMOUNT OF 20-40 MESH SAND WHICH PROVIDES AN AVERAGE LIQUID DISTANCE BETWEEN SAND GRANULES IN THE SLURRY OF 0.5-2.0 MILLIMETERS AND THEN SEPARATING THE SAND TO PRODUCE A PIGMENT DISPERSION OF 0.1-1.0 MICRON PARTICLE SIZE HAVING A VISCOSITY OF 1 TO 30 POISES, AND INTIMATELY MIXING THIS INITIAL DISPERSION WITH AT LEAST 10 TIMES ITS WEIGHT OF AN ACETONE SOLUTION OF CELLULOSE ACETATE HAVING AT LEAST 4 TIMES GREATER CONCENTRATION OF CELLULOSE ACETATE THAN THAT OF THE INITIAL DISPERSION TO PROVIDE A SPINNING SOLUTION SUITABLE FOR EXTRUSION TO FORM DELUSTERED FILMANENTS.
Claim 2
Dependent Claim 166 words
IN THE PROCESS OF DISPERSING HARD, WHITE, INORGANIC PIGMENT IN CELLULOSE ACETATE SPRINNING SOLUTION AND SPINNING THE SOLUTION TO FORM DELUSTERED CELLULOSE ACETATE YARN, THE IMPROVEMENT FOR REDUCING THE ABRASIVENESS OF THE RESULTING YARN WHICH COMPRISES AND GRINDING A SLURRY OF THE INORGANIC PIGMENT IN AN ACETONE SOLUTION OF CELLULOSE ACETATE, CONTAINING 10-40 PARTS BY WEIGHT OF PIGMENT AND 2-6 PARTS OF CELLULOSE ACETATE PER 100 PARTS OF SLURRY, BY HIGH SPEED AGITATION WITH AN AMOUNT OF 20-40 MESH SAND WHICH PROVIDES AN AVERAGE LIQUID DISTANCE BETWEEN SAND GRANULES IN THE SLURRY OF 0.5-2.0 MILLIMETERS AND THEN SEPARATING THE SAND TO PRODUCE A PIGMENT DISPERSION OF 0.1-1.0 MICRON PARTICLE SIZE HAVING A VISCOSITY OF 1 TO 30 POISES, AND INTIMATELY MIXING THIS INITIAL DISPERSION WITH AT LEAST 10 TIMES ITS WEIGHT OF AN ACETONE SOLUTION OF CELLULOSE ACETATE HAVING AT LEAST 4 TIMES GREATER CONCENTRATION OF CELLULOSE ACETATE THAN THAT OF THE INITIAL DISPERSION TO PROVIDE A SPINNING SOLUTION SUITABLE FOR EXTRUSION TO FORM DELUSTERED FILMANENTS.

References Cited (Backward Citations)

US2581414A Cited
US2701211A Cited
US2819173A Cited
US2868662A Cited
US2855156A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1964-06-26 1964-12-26 1965-06-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1968-06-26 1968-12-26 1969-06-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1972-06-26 1972-12-26 1973-06-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag