Abstract
No abstract record available.
Inventors
- 👤 William H Kapfer
- 👤 Kronstein Max
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 15:33
CPC Classifications
C; C23; C23C; C23C22/00; C23C22/05; C23C22/06; C23C22/40
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
135 words
A PROCESS FOR APPLYING A PROTECTIVE COATING TO A MAGNESUIM SURFACE SAID PROCESS COMPRISING THE STEPS OF CLEANSING SAID SURFACE, CONTACTING THE SURFACE WITH AN AQUEOUS SOLUTION HAVING AN ELAVATED TEMPERATURE AND CONSISTING ESSENTIALLY OF 50-95 PARTS BY WEIGHT OF SODUIM PYROPHOSPHATE, 1-5 PARTS BY WEIGHT OF SODIUM FLUORIDE, AND 4-40 PARTS BY WEIGHT OF A METALLIC SALT SELECTED FROM THE GROUP CONSISTING OF CADMUIM SULFATE, COPPER SULFATE, CHRONIUM SULFATE, NICKEL SULFATE, CADMIUM CYANIDE, CHROMIC NITRATE, AND ALUMINUM NITRATE, RINSING THE SURFACE, DRYING THE SAID SURFACE IN THE AIR, IMMERSING THE SAID SURFACE IN A 5-40% BY WEIGHT AQUEOUS SOLUTION HAVING AN ELAVATED TEMPERATURE OF ONE FROM THE GROUP CONSISTING OF IRON PHOSPHATE, AMMONIUM VANADITE, AND SODIUM DICHROMATE, AND RINSING THE SURFACE SO THAT THE COATED SURFACE EXHIBITS A HIGH DEGREE OF UNIFORMITY AND STABILITY.
Claim 2
Dependent Claim
135 words
A PROCESS FOR APPLYING A PROTECTIVE COATING TO A MAGNESUIM SURFACE SAID PROCESS COMPRISING THE STEPS OF CLEANSING SAID SURFACE, CONTACTING THE SURFACE WITH AN AQUEOUS SOLUTION HAVING AN ELAVATED TEMPERATURE AND CONSISTING ESSENTIALLY OF 50-95 PARTS BY WEIGHT OF SODUIM PYROPHOSPHATE, 1-5 PARTS BY WEIGHT OF SODIUM FLUORIDE, AND 4-40 PARTS BY WEIGHT OF A METALLIC SALT SELECTED FROM THE GROUP CONSISTING OF CADMUIM SULFATE, COPPER SULFATE, CHRONIUM SULFATE, NICKEL SULFATE, CADMIUM CYANIDE, CHROMIC NITRATE, AND ALUMINUM NITRATE, RINSING THE SURFACE, DRYING THE SAID SURFACE IN THE AIR, IMMERSING THE SAID SURFACE IN A 5-40% BY WEIGHT AQUEOUS SOLUTION HAVING AN ELAVATED TEMPERATURE OF ONE FROM THE GROUP CONSISTING OF IRON PHOSPHATE, AMMONIUM VANADITE, AND SODIUM DICHROMATE, AND RINSING THE SURFACE SO THAT THE COATED SURFACE EXHIBITS A HIGH DEGREE OF UNIFORMITY AND STABILITY.
References Cited (Backward Citations)
CA518474A
Cited
US1765341A
Cited
US2030601A
Cited
US2528787A
Cited
US2564864A
Cited
GB686781A
Cited
US2665231A
Cited
DE810224C
Cited
GB726935A
Cited
US2758949A
Cited
US2864730A
Cited
US2801197A
Cited
US2859144A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1963-05-03 | 1963-11-02 | 1964-05-03 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1967-05-03 | 1967-11-02 | 1968-05-03 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1971-05-03 | 1971-11-02 | 1972-05-03 | $7700.00 | Window Closed / Lapsed |