← Back to Patent Explorer
US2922719A Expired / Lapsed US ⏱️ 0.0 years remaining

Structural clay products and method of making the same

Assignee: Zonolite Co
•
Filing: 1957-04-08
•
Granted: 1960-01-26
•
Expires: 1977-04-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Gilbert C Robinson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 06:47
CPC Classifications
C; C04; C04B; C04B33/00; C04B33/02; C04B33/04; C04B33/28; C04B33/30

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 142 words
A METHOD OF MAKING A STRUCTURAL CLAY PRODUCT, WHICH COMPRISES THE STEPS OF DISPERSING CLAY PARTICLES IN WATER TO FORM AN AQUEOUS SLIP, ADDING TO THE SLIP A DRY WATERABSORPTIVE AGGREGATE IN A SUFFICIENT QUANTITY TO DEWATER THE SLIP IN A PERIOD OF TIME GENERALLY BETWEEN ABOUT 10 AND 30 MINUTED, RAPIDLY MIXING THE AGGREGATE INTO THE SLIP IMMEDIATELY AFTER ADDING SAID AGGREGATE THERETO AND PROVIDING A MIXTURE OF POURING CONSISTENCY WHEREIN THE AGGREGATE IS ESSENTIALLY UNIFORMLY DISPERSED THROUGHOUT, RAPIDLY TRANSFERRING THE MIXTURE TO A SHAPING MOLD AND BEFORE THE AGGREGATE HAS REMOVED SUBSTANTIAL WATER FROM THE SLIP, PERMITTING THE SHAPED MIXTURE TO STAND FOR A TIME SUFFICIENT TO PERMIT SAID AGGREGATE TO ABSORB THE FREE WATER FROM SAID SLIP AND THEREBY FORM A SELF-SUSTAINING MASS, AND THEREAFTER FIRING SAID MASS AT A TEMPERATURE SUFFICIENT TO VITRIFY THE CLAY IN SAID MASS.
Claim 2
Independent Claim 142 words
A METHOD OF MAKING A STRUCTURAL CLAY PRODUCT, WHICH COMPRISES THE STEPS OF DISPERSING CLAY PARTICLES IN WATER TO FORM AN AQUEOUS SLIP, ADDING TO THE SLIP A DRY WATERABSORPTIVE AGGREGATE IN A SUFFICIENT QUANTITY TO DEWATER THE SLIP IN A PERIOD OF TIME GENERALLY BETWEEN ABOUT 10 AND 30 MINUTED, RAPIDLY MIXING THE AGGREGATE INTO THE SLIP IMMEDIATELY AFTER ADDING SAID AGGREGATE THERETO AND PROVIDING A MIXTURE OF POURING CONSISTENCY WHEREIN THE AGGREGATE IS ESSENTIALLY UNIFORMLY DISPERSED THROUGHOUT, RAPIDLY TRANSFERRING THE MIXTURE TO A SHAPING MOLD AND BEFORE THE AGGREGATE HAS REMOVED SUBSTANTIAL WATER FROM THE SLIP, PERMITTING THE SHAPED MIXTURE TO STAND FOR A TIME SUFFICIENT TO PERMIT SAID AGGREGATE TO ABSORB THE FREE WATER FROM SAID SLIP AND THEREBY FORM A SELF-SUSTAINING MASS, AND THEREAFTER FIRING SAID MASS AT A TEMPERATURE SUFFICIENT TO VITRIFY THE CLAY IN SAID MASS.

References Cited (Backward Citations)

US2079665A Cited
US2103463A Cited
US2377491A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1963-01-25 1963-07-27 1964-01-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1967-01-25 1967-07-27 1968-01-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1971-01-25 1971-07-27 1972-01-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag