← Back to Patent Explorer
US2914501A Expired / Lapsed US ⏱️ 0.0 years remaining

Reaction product of mineral oil polyisobutylene, polyethylene and resinous petroleum polymerization product

Assignee: Anaconda Wire and Cable Co
•
Filing: 1955-12-01
•
Granted: 1959-11-24
•
Expires: 1975-12-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 D Ascoli Ralph Gregory

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 12:28
CPC Classifications
C; C08; C08L; C08L91/00; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31855; Y10T428/31909; Y10T428/31928; Y10T428/31938

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 163 words
A COMPOSITION OF MATTER CONSISTING OF THE REACTION PRODUCT RESULTING FROM HEATING TO A TEMPERATURE WITHIN THE RANGE OF 200 TO 400*F. A MIXTURE MADE UP ESSENTIALLY OF 30 TO 50% BY WEIGHT OF MINERAL OIL, 2 TO 7% BY WEIGHT OF POLYISOBUTYLENE HAVING A MOLECULAR WEIGHT BETWEEN 50,000 AND 150,000, 15 TO 20% BY WEIGHT OF POLYETHYLENE HAVING A MOLECULAR WEIGHT BETWEEN 5,000 AND 20,000, AND 30 TO 40% BY WEIGHT OF A RESINOUS POLYMERIZATION PRODUCT OBTAINED BY CATALYTIC POLYMERIZATION OF A MIXTURE OF UNSATURATED MONOMERS DERIVED FROM DEEP CRACKING PETROLEUM, SAID RESIN HAVING A SOFTENING POINT (B&R) OF APPROXIMATELY 100*C., A SPECIFIC GRAVITY AT 25*C. OF .970 TO .975, A REFRACTIVE INDEX AT 20*C. OF 1.5116, AND AN ACID NUMBER LESS THAN ONE, AN IODINE VALUE (WIJS) OF 120, A BROMINE NUMBER OF 7.3 AND A MOLECULAR WEIGHT OF APPROXIMATELY 1100, SAID REACTION PRODUCT BEING CHARACTERIZED BY GOOD ADHERANCE TO A POLYETHYLENE SURFACE AND A PUTTY-LIKE PLASTICITY AT NORMAL ROOM TEMPERATURE.
Claim 2
Dependent Claim 163 words
A COMPOSITION OF MATTER CONSISTING OF THE REACTION PRODUCT RESULTING FROM HEATING TO A TEMPERATURE WITHIN THE RANGE OF 200 TO 400*F. A MIXTURE MADE UP ESSENTIALLY OF 30 TO 50% BY WEIGHT OF MINERAL OIL, 2 TO 7% BY WEIGHT OF POLYISOBUTYLENE HAVING A MOLECULAR WEIGHT BETWEEN 50,000 AND 150,000, 15 TO 20% BY WEIGHT OF POLYETHYLENE HAVING A MOLECULAR WEIGHT BETWEEN 5,000 AND 20,000, AND 30 TO 40% BY WEIGHT OF A RESINOUS POLYMERIZATION PRODUCT OBTAINED BY CATALYTIC POLYMERIZATION OF A MIXTURE OF UNSATURATED MONOMERS DERIVED FROM DEEP CRACKING PETROLEUM, SAID RESIN HAVING A SOFTENING POINT (B&R) OF APPROXIMATELY 100*C., A SPECIFIC GRAVITY AT 25*C. OF .970 TO .975, A REFRACTIVE INDEX AT 20*C. OF 1.5116, AND AN ACID NUMBER LESS THAN ONE, AN IODINE VALUE (WIJS) OF 120, A BROMINE NUMBER OF 7.3 AND A MOLECULAR WEIGHT OF APPROXIMATELY 1100, SAID REACTION PRODUCT BEING CHARACTERIZED BY GOOD ADHERANCE TO A POLYETHYLENE SURFACE AND A PUTTY-LIKE PLASTICITY AT NORMAL ROOM TEMPERATURE.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1962-11-23 1963-05-25 1963-11-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1966-11-23 1967-05-25 1967-11-24 $3760.00 Window Closed / Lapsed