Organosilicon condensation products and processes for producing them

Assignee: Siemens Schuckertwerke AG
•
Filing: 1954-07-01
•
Granted: 1959-08-25
•
Expires: 1974-07-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Schwarz Robert
  • 👤 Kuchen Wilhelm
  • 👤 Weigel Fritz

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 08:15
CPC Classifications
C; C08; C08G; C08G77/00

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 151 words
THE METHOD OF PRODUCING HEAT-HARDENABLE RESINOUS PRODUCTS, COMPRISING HEATING AN ADMIXTURE OF AN AROMATIC SILIXCIC ACID ESTER AND AT LEAST ONE ALIPHATIC POLYHYDROXY COMPOUND, AN ISOCYANATE TAKEN FROM THE GROUP CONSISTING OF ALKYLENE AND ARYLENE POLYISOCYANATES BEING ADDED TO THE SAID ADMIXTURE TO REACT WITH THE SAID POLYHYDROXY COMPOUND, THE POLYISOCYANATE ADDITION BEING IN AN AMOUNT TO LEAVE AT LEAST 0.1 MOLE OF HYDROXYL GROUPS PER MOLE OF AROMATIC SILICATE, THERE BEING A RA TIO OF 0.1 TO ABOUT 0.33 MOLE OF THE AROMATIC SILICIC ACID ESTER PER MOLE OF HYDROXYL GROUPS IN THE POLYHYDROXY COMPOUND AND A MAXIMUM TOTAL MOLE RATIO OF THE SILICATE ACID ESTER AND POLVISOCYANATE OF ABOUT 0.66 PER MOLE OF THE HYDROXYL GROUPS IN SAID POLYHYDROXYL COMPOUND, CONTINUING THE HEATING UNTIL SEPARATION OF THE COMPONENTS UPON COOLING SUBSTANTIALLY CEASES, AND SEPARATING LIBERATED AROMATIC ALCOHOL FROM THE REACTION PRODUCT COMPRISING A SUBSTANTIAL RATIO OF FREE HYDROXYL GROUPS.
Claim 2
Independent Claim 151 words
THE METHOD OF PRODUCING HEAT-HARDENABLE RESINOUS PRODUCTS, COMPRISING HEATING AN ADMIXTURE OF AN AROMATIC SILIXCIC ACID ESTER AND AT LEAST ONE ALIPHATIC POLYHYDROXY COMPOUND, AN ISOCYANATE TAKEN FROM THE GROUP CONSISTING OF ALKYLENE AND ARYLENE POLYISOCYANATES BEING ADDED TO THE SAID ADMIXTURE TO REACT WITH THE SAID POLYHYDROXY COMPOUND, THE POLYISOCYANATE ADDITION BEING IN AN AMOUNT TO LEAVE AT LEAST 0.1 MOLE OF HYDROXYL GROUPS PER MOLE OF AROMATIC SILICATE, THERE BEING A RA TIO OF 0.1 TO ABOUT 0.33 MOLE OF THE AROMATIC SILICIC ACID ESTER PER MOLE OF HYDROXYL GROUPS IN THE POLYHYDROXY COMPOUND AND A MAXIMUM TOTAL MOLE RATIO OF THE SILICATE ACID ESTER AND POLVISOCYANATE OF ABOUT 0.66 PER MOLE OF THE HYDROXYL GROUPS IN SAID POLYHYDROXYL COMPOUND, CONTINUING THE HEATING UNTIL SEPARATION OF THE COMPONENTS UPON COOLING SUBSTANTIALLY CEASES, AND SEPARATING LIBERATED AROMATIC ALCOHOL FROM THE REACTION PRODUCT COMPRISING A SUBSTANTIAL RATIO OF FREE HYDROXYL GROUPS.

References Cited (Backward Citations)

FR923420A Cited
US2048799A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1962-08-24 1963-02-23 1963-08-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1966-08-24 1967-02-23 1967-08-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1970-08-24 1971-02-23 1971-08-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag