Method of cold rolling ferrous strip stock
Assignee: Parker Rust Proof Co
•
Filing: 1956-01-25
•
Granted: 1959-04-28
•
Expires: 1976-01-25
Abstract
No abstract record available.
Inventors
- 👤 Walter R Cavanagh
- 👤 Robert C Gibson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 07:37
CPC Classifications
C; C23; C23C; C23C22/00; C23C22/05; C23C22/06; C23C22/07; C23C22/08; C23C22/22; B; B21; B21B; B21B1/00; B21B1/22; C23C22/12
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
142 words
A METHOD FOR TREATING CONTINUOUS FERROUS STRIP STOCK WHICH COMPRISES THE STEPS OF PICKLING THE STRIP, CONTACTING THE SAID PICKLED STRIP WHILE THE SAME IS MOVING WITH AN AQUEOUS ACIDIC ZINC PHOSPHATE COATING SOLUTION COMPRISING AS THE ESSENTIAL COATING PRODUCING INGREDIENTS ZINC IN AN AMOUNT IN THE RANGE OF 0.05%-1.5% BY WEIGHT, 0.4 TO ABOUT 2.5% PO4 AND AN OXIDIZING AGENT OTHER THAN CHLORATE IN AN AMOUNT SUFFICIENT TO PRODUCE A COATING WEIGHT OF AT LEAST 50 MG. PER SQUARE FOOT IN NOT MORE THAN 10 SECONDS, AND REGULATING THE TIME OF CONTACT OF SAID PICKLED STRIP WITH SAID SOLUTION SO AS TO PRODUCE A COATING WHICH HAS A WEIGHT IN THE RANGE OF ABOUT 50 MG./ SQ. FT TO ABOUT 1000 MG./SQ.FT. AND WHICH VARIES FROM THE AVERAGE COATING WEIGHT PREVALENT ON SAID STRIP BY NOT MORE THAN ABOUT 200 MG./SQ.FT.
Claim 2
Independent Claim
142 words
A METHOD FOR TREATING CONTINUOUS FERROUS STRIP STOCK WHICH COMPRISES THE STEPS OF PICKLING THE STRIP, CONTACTING THE SAID PICKLED STRIP WHILE THE SAME IS MOVING WITH AN AQUEOUS ACIDIC ZINC PHOSPHATE COATING SOLUTION COMPRISING AS THE ESSENTIAL COATING PRODUCING INGREDIENTS ZINC IN AN AMOUNT IN THE RANGE OF 0.05%-1.5% BY WEIGHT, 0.4 TO ABOUT 2.5% PO4 AND AN OXIDIZING AGENT OTHER THAN CHLORATE IN AN AMOUNT SUFFICIENT TO PRODUCE A COATING WEIGHT OF AT LEAST 50 MG. PER SQUARE FOOT IN NOT MORE THAN 10 SECONDS, AND REGULATING THE TIME OF CONTACT OF SAID PICKLED STRIP WITH SAID SOLUTION SO AS TO PRODUCE A COATING WHICH HAS A WEIGHT IN THE RANGE OF ABOUT 50 MG./ SQ. FT TO ABOUT 1000 MG./SQ.FT. AND WHICH VARIES FROM THE AVERAGE COATING WEIGHT PREVALENT ON SAID STRIP BY NOT MORE THAN ABOUT 200 MG./SQ.FT.
References Cited (Backward Citations)
US1279101A
Cited
US2105015A
Cited
US2230319A
Cited
US2164042A
Cited
US2314887A
Cited
US2298312A
Cited
US2293716A
Cited
US2351605A
Cited
US2462196A
Cited
US2479564A
Cited
US2476345A
Cited
US2540314A
Cited
US2522176A
Cited
US2516008A
Cited
US2608496A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1962-04-27 | 1962-10-27 | 1963-04-28 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1966-04-27 | 1966-10-27 | 1967-04-28 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1970-04-27 | 1970-10-27 | 1971-04-28 | $7700.00 | Window Closed / Lapsed |