Abstract
No abstract record available.
Inventors
- 👤 Thomas C Morris
- 👤 Adolph M Chaplick
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-25 00:16
CPC Classifications
C; C09; C09J; C09J163/00; A; A43; A43D; A43D25/00; A43D25/18; B; B05; B05C; B05C11/00; B05C11/10; B05C11/1042; B05C5/00; B05C5/001; C08; C08G; C08G69/00; C08G69/02; C08G69/26; C08G69/34; C08L; C08L63/00; C08L77/00; C08L77/06; C08L77/08; C09D; C09D5/00; C09D5/002; C09J123/00; C09J123/02; C09J177/00; C09J177/06; C09J177/08; C09J5/00; C09J5/06; C09J7/00; C09J7/10; C09J9/00; C09J9/005; C08L2666/00; C08L2666/02; C08L2666/14; C08L2666/22
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
173 words
A PERMANENTLY FUSIBLE, THERMOPLASTIC ADHESIVE COMPRISING A RESINOUS POLYAMIDE REACTION PRODUCT OF A POLYMERIC POLYENE FAT ACID AND AN ALKYLENE POLYAMINE PROSSESSING AT LEAST TWO PRIMARY AMINO GROUPS, AND A MINOR PROPORTION OF A RESINOUS POLYEPOXIDE REACTED WITH SAID POLYAMIDE, SAID POLYAMIDE HAVING AN AMINE VALUE IN EXCESS OF 1 MG. OF -NH2 PER GRAM OF POLYAMIDE, AND SAID RESINOUS POLYPEOXIDE BEING A RESINOUS GLYCIDYL POLYETHER OF A MEMBER OF THE GROUP CONSISTING OF POLYHYDRIC PHENOLS, POLYHYDRIC ALCOHOLS AND MIXTURES OF THESE, SAID RESINOUS POLYEPOXIDE BEING PRESENT IN AMOUNTS FROM 1/4% BY WEIGHT BASED ON THE WEIGHT OF SAID POLYAMIDE TO NOT MORE THAN ABOUT 90% OF THAT QUANTITY WHICH WILL FORM IN A MIXTURE CONSISTING OF THE POLYAMIDE AND POLYEPOXIDE HEATED FOR ONE-HALF HOUR AT 150*C. A GEL STRUCTURE IN WHICH A 3/10" STEEL BALL WILL JUST BEGIN TO FALL ERRATICALLY THROUGH A BODY OF THE RESIN IN A GLASS TUBE 1" IN DIAMETER AT A TEMPERATURE OF 150*C., SAID POLYEPOXIDE SERVING TO INCREASE THE DIMENSIONAL STABILITY AND STRENGTH OF THE COMPOSITION.
Claim 2
Dependent Claim
173 words
A PERMANENTLY FUSIBLE, THERMOPLASTIC ADHESIVE COMPRISING A RESINOUS POLYAMIDE REACTION PRODUCT OF A POLYMERIC POLYENE FAT ACID AND AN ALKYLENE POLYAMINE PROSSESSING AT LEAST TWO PRIMARY AMINO GROUPS, AND A MINOR PROPORTION OF A RESINOUS POLYEPOXIDE REACTED WITH SAID POLYAMIDE, SAID POLYAMIDE HAVING AN AMINE VALUE IN EXCESS OF 1 MG. OF -NH2 PER GRAM OF POLYAMIDE, AND SAID RESINOUS POLYPEOXIDE BEING A RESINOUS GLYCIDYL POLYETHER OF A MEMBER OF THE GROUP CONSISTING OF POLYHYDRIC PHENOLS, POLYHYDRIC ALCOHOLS AND MIXTURES OF THESE, SAID RESINOUS POLYEPOXIDE BEING PRESENT IN AMOUNTS FROM 1/4% BY WEIGHT BASED ON THE WEIGHT OF SAID POLYAMIDE TO NOT MORE THAN ABOUT 90% OF THAT QUANTITY WHICH WILL FORM IN A MIXTURE CONSISTING OF THE POLYAMIDE AND POLYEPOXIDE HEATED FOR ONE-HALF HOUR AT 150*C. A GEL STRUCTURE IN WHICH A 3/10" STEEL BALL WILL JUST BEGIN TO FALL ERRATICALLY THROUGH A BODY OF THE RESIN IN A GLASS TUBE 1" IN DIAMETER AT A TEMPERATURE OF 150*C., SAID POLYEPOXIDE SERVING TO INCREASE THE DIMENSIONAL STABILITY AND STRENGTH OF THE COMPOSITION.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1962-01-05 | 1962-07-07 | 1963-01-06 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1966-01-05 | 1966-07-07 | 1967-01-06 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1970-01-05 | 1970-07-07 | 1971-01-06 | $7700.00 | Window Closed / Lapsed |