Method of electrolytically depositing smooth layers of tin

Assignee: Dr Ing Max Schloetter GmbH and Co KG
•
Filing: 1957-01-10
•
Granted: 1958-08-05
•
Expires: 1977-01-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Frick Wolfgang
  • 👤 Geldbach Alfred
  • 👤 Korpiun Joachim
  • 👤 Sedlacek Friedrich

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 19:26
CPC Classifications
C; C25; C25D; C25D3/00; C25D3/02; C25D3/30; C25D3/32

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 56 words
IN THE ELECTROLYTIC DEPOSITION OF TIN AS A SMOOTH LAYER, THE STEP COMPRISING DEPOSITING SAID TIN FROM AN ACID TIN ELECTROLYTE WHICH CONTAINS A FLAVONOL COMPOUND IN AN AMOUNT SUFFICIENT TO CAUSE DEPOSITION OF A SMOOTH TIN LAYER AND IMPROVEMENT OF THE THROWING POWER OF THE ELECTROLYTE ON OPERATION AT LOW VOLTAGES WITH HIGH CURRENT DENSITIES.
Claim 2
Dependent Claim 56 words
IN THE ELECTROLYTIC DEPOSITION OF TIN AS A SMOOTH LAYER, THE STEP COMPRISING DEPOSITING SAID TIN FROM AN ACID TIN ELECTROLYTE WHICH CONTAINS A FLAVONOL COMPOUND IN AN AMOUNT SUFFICIENT TO CAUSE DEPOSITION OF A SMOOTH TIN LAYER AND IMPROVEMENT OF THE THROWING POWER OF THE ELECTROLYTE ON OPERATION AT LOW VOLTAGES WITH HIGH CURRENT DENSITIES.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1961-08-04 1962-02-03 1962-08-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1965-08-04 1966-02-03 1966-08-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1969-08-04 1970-02-03 1970-08-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag