Abstract

No abstract record available.

Inventors

  • 👤 Haugen Ole Wilhelm

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 14:06
CPC Classifications
C; C25; C25C; C25C1/00; C25C1/20

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 160 words
IN A PROCESS FOR THE RECOVERY OF PRECIOUS METALS, ESPECIALLY GOLD AND SILVER, BY THE CYANIDE-LEACHING PROCESS, THAT IMPROVEMENT IN LEACHING THE PRECIOUS METAL-CONTAINING STARTING MATERIAL IN A FINE STATE OF SUBDIVISION COM PRISING THE FOLLOWING STEPS: EXPOSING THE STARTING MATERIAL TO A SOLUTION CONTAINING ABOUT 10,000 GRAMS OF AN ALKALI METAL CYANIDE, 150 GRAMS OF AN ALKALI METAL HYDROXIDE AND 250 GRAMS OF SLAKED LIME PRE CUBIC METER OF SAID SOLUTION, IN THE PRESENCE OF OXYGEN, THE RATIO OF STARTING MATERIAL TO SAID SOLUTION BEING ABOUT BETWEEN 1.5 TO 1 TO ABOUT 4 TO 1 AND SIMULTANEOUSLY PASSING DIRECT ELECTRIC CURRENT AT A CONSTANT VOLTAGE OF FROM 6 TO 8 VOLTS THROUGH SAID SOLUTION FOR A PERIOD OF ABOUT 4 TO 8 HOURS WITH A CURRENT CONSUMPTION OF ABOUT 1 TO 2 AMPERES PER TON OF DRY STARTING MATERIAL, WHEREBY SAID STARTING MATERIAL IS LEACHED OF ITS PRECIOUS METAL-CONTAINING VALUES IN ACCORDANCE WITH THE EQUATION BELOW, EXEMPLIFIED BY GOLD:
Claim 2
Dependent Claim 160 words
IN A PROCESS FOR THE RECOVERY OF PRECIOUS METALS, ESPECIALLY GOLD AND SILVER, BY THE CYANIDE-LEACHING PROCESS, THAT IMPROVEMENT IN LEACHING THE PRECIOUS METAL-CONTAINING STARTING MATERIAL IN A FINE STATE OF SUBDIVISION COM PRISING THE FOLLOWING STEPS: EXPOSING THE STARTING MATERIAL TO A SOLUTION CONTAINING ABOUT 10,000 GRAMS OF AN ALKALI METAL CYANIDE, 150 GRAMS OF AN ALKALI METAL HYDROXIDE AND 250 GRAMS OF SLAKED LIME PRE CUBIC METER OF SAID SOLUTION, IN THE PRESENCE OF OXYGEN, THE RATIO OF STARTING MATERIAL TO SAID SOLUTION BEING ABOUT BETWEEN 1.5 TO 1 TO ABOUT 4 TO 1 AND SIMULTANEOUSLY PASSING DIRECT ELECTRIC CURRENT AT A CONSTANT VOLTAGE OF FROM 6 TO 8 VOLTS THROUGH SAID SOLUTION FOR A PERIOD OF ABOUT 4 TO 8 HOURS WITH A CURRENT CONSUMPTION OF ABOUT 1 TO 2 AMPERES PER TON OF DRY STARTING MATERIAL, WHEREBY SAID STARTING MATERIAL IS LEACHED OF ITS PRECIOUS METAL-CONTAINING VALUES IN ACCORDANCE WITH THE EQUATION BELOW, EXEMPLIFIED BY GOLD:

References Cited (Backward Citations)

US775597A Cited
US998749A Cited
US1082596A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1961-07-14 1962-01-13 1962-07-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1965-07-14 1966-01-13 1966-07-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1969-07-14 1970-01-13 1970-07-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag