Process of plating glass fiber rovings with iron metal
Assignee: Commonwealth Engineering Company of Ohio
•
Filing: 1952-12-09
•
Granted: 1957-12-31
•
Expires: 1972-12-09
Abstract
No abstract record available.
Inventors
- 👤 Herman R Nack
- 👤 John R Whitacre
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 12:21
CPC Classifications
C; C23; C23C; C23C16/00; C23C16/06; C23C16/16; C03; C03C; C03C25/00; C03C25/10; C03C25/42; C03C25/46; C23C16/44; C23C16/54; C23C16/545; Y; Y10; Y10S; Y10S264/00; Y10S264/19; Y10T; Y10T428/00; Y10T428/29; Y10T428/2913; Y10T428/2933; Y10T428/294; Y10T428/2956
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
151 words
IN A PROCESS OF PLATING GLASS FIBER ROVINGS WITH IRON METAL AS THE SAME IS PASSED THROUGH A PLATING CHAMBER WHICH PROCESS COMPRISES MOVING THE GLASS FIBER IN THE FORM OF UNTWISTED PARALLEL STRANDS INTO A CONFINED ZONE FILLED WITH DRY AIR HEATED TO AT LEAST 150*F., AND THENCE THROUGH A PLATING AREA SURROUNDED BY SAID CONFINED ZONE EXCLUDING OXYGEN AND WATER VAPOR FROM THE PLATING AREA BY FILLING THE SAME WITH DRY INERT GAS, INTRODUCING GASEOUS IRON PENTACARBONYL INTO SAID PLATING AREA TOGETHER WITH SAID INERT GAS A CARRIER, VIBRATING THE ROVING TO CAUSE TEMPORARY SEPARATION OF THE ROVING STRANDS EXPOSING THE SAME TO GASEOUS IRON CARBONYL, AND HEATING THE THUS EXPOSED STRANDS OF GLASS FIBER AT A TEMPERATURE TO CAUSE DECOMPOSITION OF THE IRON CARBONYL AND DEPOSITION OF METALLIC IRON ON THE SURFACE OF THE FIBERS, AND THEREAFTER GRADUALLY COOLING THE RESULTANT IRON-COATED GLASS FIBERS WITHIN SAID CONFINED ZONE.
Claim 2
Dependent Claim
151 words
IN A PROCESS OF PLATING GLASS FIBER ROVINGS WITH IRON METAL AS THE SAME IS PASSED THROUGH A PLATING CHAMBER WHICH PROCESS COMPRISES MOVING THE GLASS FIBER IN THE FORM OF UNTWISTED PARALLEL STRANDS INTO A CONFINED ZONE FILLED WITH DRY AIR HEATED TO AT LEAST 150*F., AND THENCE THROUGH A PLATING AREA SURROUNDED BY SAID CONFINED ZONE EXCLUDING OXYGEN AND WATER VAPOR FROM THE PLATING AREA BY FILLING THE SAME WITH DRY INERT GAS, INTRODUCING GASEOUS IRON PENTACARBONYL INTO SAID PLATING AREA TOGETHER WITH SAID INERT GAS A CARRIER, VIBRATING THE ROVING TO CAUSE TEMPORARY SEPARATION OF THE ROVING STRANDS EXPOSING THE SAME TO GASEOUS IRON CARBONYL, AND HEATING THE THUS EXPOSED STRANDS OF GLASS FIBER AT A TEMPERATURE TO CAUSE DECOMPOSITION OF THE IRON CARBONYL AND DEPOSITION OF METALLIC IRON ON THE SURFACE OF THE FIBERS, AND THEREAFTER GRADUALLY COOLING THE RESULTANT IRON-COATED GLASS FIBERS WITHIN SAID CONFINED ZONE.
References Cited (Backward Citations)
US1072904A
Cited
GB306902A
Cited
US1998060A
Cited
US2304182A
Cited
US2344138A
Cited
US2325126A
Cited
US2428654A
Cited
US2616165A
Cited
US2542819A
Cited
US2622041A
Cited
US2577936A
Cited
US2584660A
Cited
US2622043A
Cited
US2602033A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1960-12-30 | 1961-07-01 | 1961-12-31 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1964-12-30 | 1965-07-01 | 1965-12-31 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1968-12-30 | 1969-07-01 | 1969-12-31 | $7700.00 | Window Closed / Lapsed |