← Back to Patent Explorer
US2809905A Expired / Lapsed US ⏱️ 0.0 years remaining

Melting and refining metals

Assignee: National Research Development Corp UK
•
Filing: 1956-12-21
•
Granted: 1957-10-15
•
Expires: 1976-12-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Davis Michael
  • 👤 Lever Reginald Frank

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 06:38
CPC Classifications
H; H01; H01J; H01J37/00; H01J37/30; H01J37/305; C; C30; C30B; C30B13/00; C30B13/08; C30B13/10; C30B13/12; C30B13/16; C30B13/22; C30B29/00; C30B29/10; C30B29/16; C30B29/20; Y; Y10; Y10S; Y10S117/00; Y10S117/90; Y10S117/905; Y10S117/911; Y10S148/00; Y10S148/074; Y10S164/00; Y10S164/04; Y10T; Y10T117/00; Y10T117/10; Y10T117/1024; Y10T117/1076; Y10T117/1088; Y10T279/00; Y10T279/17; Y10T279/17128; Y10T279/17136; Y10T279/17153

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 145 words
A METHOD OF REFINING A REFRACTORY MATERIAL WHICH IS STABLE WHEN MOLTEN AND HAS A NEGLIGIBLE VAPOUR PRESSURE AT ITS MELTING POINT BUT CONTAINS AN IMPURITY OF HIGHER SOLUBILITY IN THE MATERIAL WHEN MOLTEN THAN IN THE MATERIAL IN ITS SOLID STATE, WHICH METHOD COMPRISES THE STEPS OF SUPPORTING A SOLID ROD OF THE MATERIAL IN AN EVACUABLE ENCLOSURE, CONTAINING AN ELECTRON GUN, EVACUATING SAID ENCLOSURE, HEATING THE ROAD OF MATERIAL IN THE EVACUATED CLOSURE BY ELECTRON BOMBARDMENT FROM SAID GUN CONFINED TO A LIMITED ZONE OF THE ROD TO MELT THE MATERIAL AT SAID ZONE WITHOUT CAUSING THE MELT TO RUN FROM THE ROD, AND TRAVERSING SAID ROD AND SAID GUN RELATIVE TO ONE ANOTHER TO MOVE THE MELTED ZONE ALONG THE ROD TO COLLECT IN SAID ZONE THE IMPURITIES SOLUBLE THEREIN AND THEREBY TO TRNASFER THEM TO AN END PORTION OF THE ROD.
Claim 2
Independent Claim 145 words
A METHOD OF REFINING A REFRACTORY MATERIAL WHICH IS STABLE WHEN MOLTEN AND HAS A NEGLIGIBLE VAPOUR PRESSURE AT ITS MELTING POINT BUT CONTAINS AN IMPURITY OF HIGHER SOLUBILITY IN THE MATERIAL WHEN MOLTEN THAN IN THE MATERIAL IN ITS SOLID STATE, WHICH METHOD COMPRISES THE STEPS OF SUPPORTING A SOLID ROD OF THE MATERIAL IN AN EVACUABLE ENCLOSURE, CONTAINING AN ELECTRON GUN, EVACUATING SAID ENCLOSURE, HEATING THE ROAD OF MATERIAL IN THE EVACUATED CLOSURE BY ELECTRON BOMBARDMENT FROM SAID GUN CONFINED TO A LIMITED ZONE OF THE ROD TO MELT THE MATERIAL AT SAID ZONE WITHOUT CAUSING THE MELT TO RUN FROM THE ROD, AND TRAVERSING SAID ROD AND SAID GUN RELATIVE TO ONE ANOTHER TO MOVE THE MELTED ZONE ALONG THE ROD TO COLLECT IN SAID ZONE THE IMPURITIES SOLUBLE THEREIN AND THEREBY TO TRNASFER THEM TO AN END PORTION OF THE ROD.

References Cited (Backward Citations)

US2771568A Cited
US2778926A Cited
US2739088A Cited
US2792317A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1960-10-14 1961-04-15 1961-10-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1964-10-14 1965-04-15 1965-10-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1968-10-14 1969-04-15 1969-10-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag