← Back to Patent Explorer
US2779974A Expired / Lapsed US ⏱️ 0.0 years remaining

Preparation of highly polymeric material in a form suitable for transport

Assignee: Acordis UK Ltd
•
Filing: 1952-08-20
•
Granted: 1957-02-05
•
Expires: 1972-08-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Billing Joseph
  • 👤 Bostock Cyril

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 12:09
CPC Classifications
C; C08; C08B; C08B3/00; C08B3/22; Y; Y10; Y10S; Y10S264/00; Y10S264/64; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31971

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 143 words
PROCESS FOR CONVERTING PARTICULATE CELLULOSE ACETATE OF BULK DENSITY BELOW 30 LB. PER CUBIC FOOT INTO A FORM MORE SUITABLE FOR TRANSPORT, WHICH COMPRISES COMPRESSING THE CELLULOSE ACETATE, WHILE IT IS FREE SOLVENTS AND SOFTENING AGENTS AND AT A TEMPERATURE BELOW ITS THERMAL SOFTENING TEMPERATURE, INTO A BLOCK HAVING A DENSITY BETWEEN 50% AND 75% OF THE TRUE DENSITY OF THE CELLULOSE ACETATE, APPLYING A VOLATILE SOLVENT FOR THE CELLULOSE ACETATE TO THE SURFACES OF THE BLOCK, ALLOWING THE SOLVENT TO PENETRATE THE BLOCK A CONTINUOUS SKIN OF THICKNESS BETWEEN 0.005 REMOVING THE SOLVENT BY EVAPORATION, THEREBY FORMING ON THE BLOCK A CONTINUOUS SKIN OF THICKESS BETWEE 0.005 AND 0.1 INCH TO THUS PRODUCE A BLOCK WHICH IS RESISTANT TO THE ORDINARY DISRUPTIVE FORCES ATTENDING TRANSPORT BUT WHCIH CAN BE READILY BROKEN DOWN BY IMPACT ATTRITION IN A HAMMER MILL OR LIKE DEVICE.
Claim 2
Dependent Claim 143 words
PROCESS FOR CONVERTING PARTICULATE CELLULOSE ACETATE OF BULK DENSITY BELOW 30 LB. PER CUBIC FOOT INTO A FORM MORE SUITABLE FOR TRANSPORT, WHICH COMPRISES COMPRESSING THE CELLULOSE ACETATE, WHILE IT IS FREE SOLVENTS AND SOFTENING AGENTS AND AT A TEMPERATURE BELOW ITS THERMAL SOFTENING TEMPERATURE, INTO A BLOCK HAVING A DENSITY BETWEEN 50% AND 75% OF THE TRUE DENSITY OF THE CELLULOSE ACETATE, APPLYING A VOLATILE SOLVENT FOR THE CELLULOSE ACETATE TO THE SURFACES OF THE BLOCK, ALLOWING THE SOLVENT TO PENETRATE THE BLOCK A CONTINUOUS SKIN OF THICKNESS BETWEEN 0.005 REMOVING THE SOLVENT BY EVAPORATION, THEREBY FORMING ON THE BLOCK A CONTINUOUS SKIN OF THICKESS BETWEE 0.005 AND 0.1 INCH TO THUS PRODUCE A BLOCK WHICH IS RESISTANT TO THE ORDINARY DISRUPTIVE FORCES ATTENDING TRANSPORT BUT WHCIH CAN BE READILY BROKEN DOWN BY IMPACT ATTRITION IN A HAMMER MILL OR LIKE DEVICE.

References Cited (Backward Citations)

US1770573A Cited
US2142968A Cited
US2209940A Cited
US2282421A Cited
US2346210A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1960-02-05 1960-08-06 1961-02-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1964-02-05 1964-08-06 1965-02-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1968-02-05 1968-08-06 1969-02-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags