← Back to Patent Explorer
US2762703A Expired / Lapsed US ⏱️ 0.0 years remaining

Processes for treating materials containing nickel and iron

Assignee: Bethlehem Steel Corp
•
Filing: 1953-12-23
•
Granted: 1956-09-11
•
Expires: 1973-12-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Edgar B Mancke

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 20:26
CPC Classifications
C; C22; C22B; C22B23/00; C22B23/04; C22B23/0407; C22B23/0415; C22B23/0438; C22B3/00; C22B3/04; C22B3/06; C22B3/065; Y; Y02; Y02P; Y02P10/00; Y02P10/20

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 122 words
A PROCESS OF TREATING IRON ORE CONTAINING NICKEL, COMPRISING THE STEPS OF MIXING THE MATERIAL WITH AN AQUEOUS SOLUTION OF NITRIC ACID IN AN AMOUNT AT LEAST SUFFICIENT TO COMBINE WITH THE MAJOR PORTION OF THE IRON AND ALSO COMBINE WITH THE NON-FERROUS CONSTITUENTS OF THE MATERIAL CAPABLE OF BEING DISSOLVED BY NITRIC ACID, MAINTAINING THE ACID AND MATERIAL IN CONTACT A SUFFICIENT PERIOD OF TIME TO DISSOLVE THE MAJOR PORTION OF THE IRON AND NICKEL OF THE MATERIAL, SEPARATING THE SOLUTION FROM THE UNDISSOLVED PORTION OF THE MATERIAL, AND AUTOCLAVING THE SOLUTION AT A TEMPERATURE BETWEEN 365* F. AND 650* F. TO OBTAIN A SOLID PHASE CONTAINING IRON AND A SOLUTION CONTAINING THE MAJOR PORTION OF THE NICKEL OF THE MATERIAL.
Claim 2
Dependent Claim 122 words
A PROCESS OF TREATING IRON ORE CONTAINING NICKEL, COMPRISING THE STEPS OF MIXING THE MATERIAL WITH AN AQUEOUS SOLUTION OF NITRIC ACID IN AN AMOUNT AT LEAST SUFFICIENT TO COMBINE WITH THE MAJOR PORTION OF THE IRON AND ALSO COMBINE WITH THE NON-FERROUS CONSTITUENTS OF THE MATERIAL CAPABLE OF BEING DISSOLVED BY NITRIC ACID, MAINTAINING THE ACID AND MATERIAL IN CONTACT A SUFFICIENT PERIOD OF TIME TO DISSOLVE THE MAJOR PORTION OF THE IRON AND NICKEL OF THE MATERIAL, SEPARATING THE SOLUTION FROM THE UNDISSOLVED PORTION OF THE MATERIAL, AND AUTOCLAVING THE SOLUTION AT A TEMPERATURE BETWEEN 365* F. AND 650* F. TO OBTAIN A SOLID PHASE CONTAINING IRON AND A SOLUTION CONTAINING THE MAJOR PORTION OF THE NICKEL OF THE MATERIAL.

References Cited (Backward Citations)

US981451A Cited
GB188865A Cited
US1590525A Cited
GB386288A Cited
US2643204A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1959-09-11 1960-03-12 1960-09-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1963-09-11 1964-03-12 1964-09-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1967-09-11 1968-03-12 1968-09-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag