Abstract

No abstract record available.

Inventors

  • 👤 Schuyler A Herres
  • 👤 Ernest G Kendall

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 12:58
CPC Classifications
C; C22; C22B; C22B34/00; C22B34/10; C22B34/14; C22B34/12; C22B34/1295

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 121 words
A PROCESS FOR PURIFYING A REFRACTORY METAL CONTAMINATED WITH A REDUCING METAL AND A HALIDE OF SAID REDUCING METAL WHICH COMPRISES; COMMINUTING SAID METAL TO A PARTICLE SIZE OF LESS THAN ABOUT 4 MESH, WASHING SAID COMMINUTED METAL, WITHOUT INTERMEDIATE ACID TREATMENT, EMPLOYING A SPRAY OF EXCESS WATER THEREBY TO DISSOLVE REDUCING METAL CHLORIDE AND TO MAINTAIN THE TEMPEATURE OF SAID REFRACTORY METAL BELOW ABOUT 30* F., SUBSEQUENTLY IMMERSING SAID WASHED METAL IN AN AQUEOUS ACID SOLUTION UNTIL THE REDUCING METAL IS DISSOLVED, SAID ACID SOLUTION BEING OF SUCH STRENGTH AND IN AMOUNT THAT THE HYDROGEN ION CONTENT OF THE SPENT ACID AFTER TREATMENT OF THE METAL IS NOT LOWER THAN 0.1 GRAM PER LITER, AND RINSING AND DRYING SAID METAL.
Claim 2
Dependent Claim 121 words
A PROCESS FOR PURIFYING A REFRACTORY METAL CONTAMINATED WITH A REDUCING METAL AND A HALIDE OF SAID REDUCING METAL WHICH COMPRISES; COMMINUTING SAID METAL TO A PARTICLE SIZE OF LESS THAN ABOUT 4 MESH, WASHING SAID COMMINUTED METAL, WITHOUT INTERMEDIATE ACID TREATMENT, EMPLOYING A SPRAY OF EXCESS WATER THEREBY TO DISSOLVE REDUCING METAL CHLORIDE AND TO MAINTAIN THE TEMPEATURE OF SAID REFRACTORY METAL BELOW ABOUT 30* F., SUBSEQUENTLY IMMERSING SAID WASHED METAL IN AN AQUEOUS ACID SOLUTION UNTIL THE REDUCING METAL IS DISSOLVED, SAID ACID SOLUTION BEING OF SUCH STRENGTH AND IN AMOUNT THAT THE HYDROGEN ION CONTENT OF THE SPENT ACID AFTER TREATMENT OF THE METAL IS NOT LOWER THAN 0.1 GRAM PER LITER, AND RINSING AND DRYING SAID METAL.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1959-04-03 1959-10-03 1960-04-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1963-04-03 1963-10-03 1964-04-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1967-04-03 1967-10-03 1968-04-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag