← Back to Patent Explorer
US2739932A Expired / Lapsed US ⏱️ 0.0 years remaining

Electrodepositing chromium on aluminum

Assignee: Individual
•
Filing: 1952-09-05
•
Granted: 1956-03-27
•
Expires: 1972-09-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Clarence W Forestek

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 01:37
CPC Classifications
C; C25; C25D; C25D5/00; C25D5/34; C25D5/42; C25D5/44

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 120 words
A METHOD OF ELECTRODEPOSITING CHROMIUM ON THE SURFACE OF AN ALUMINUM MEMBER; COMPRISING THE STEPS OF; CHEMICALLY REPLACING THE OXIDE FILM ON SAID SURFACE WITH A PROTECTIVE COATING OF ZINCATE TO PREVENT RE-OXIDATION UPON CONTACT WITH THE ATMOSPHERE; REMOVING SAID PROTECTIVE COATING AND SIMULTANEOUSLY PROVIDING AN ELECTRODEPOSIT OF CHROMIUM, ADHERED DIRECTLY TO SAID ALUMINUM SURFACE BY ELECTROLYSIS, OF SAID ALUMINUM MEMBER AT CONSTANT TEMPERATURE, IN A CONCENTRATED ELECTROLYTIC SOLUTION INCLUDING CHROMIC ACID AND SULFURIC ACID, SAID CONSTANT TEMPERATURE BEING BETWEEN 90* F. AND 120* F. SAID CHROMIC ACID BEING PRESENT IN CONCENTRATIONS RANGING FROM 40 TO 60 OUNCES PER GALLON OF SOLUTION; AND SAID SULFURIC ACID BEING PRESENT IN CONCENTRATIONS RANGING FROM 40 TO 60 OUNCES PER GALLON OF SOLUTION.
Claim 2
Independent Claim 120 words
A METHOD OF ELECTRODEPOSITING CHROMIUM ON THE SURFACE OF AN ALUMINUM MEMBER; COMPRISING THE STEPS OF; CHEMICALLY REPLACING THE OXIDE FILM ON SAID SURFACE WITH A PROTECTIVE COATING OF ZINCATE TO PREVENT RE-OXIDATION UPON CONTACT WITH THE ATMOSPHERE; REMOVING SAID PROTECTIVE COATING AND SIMULTANEOUSLY PROVIDING AN ELECTRODEPOSIT OF CHROMIUM, ADHERED DIRECTLY TO SAID ALUMINUM SURFACE BY ELECTROLYSIS, OF SAID ALUMINUM MEMBER AT CONSTANT TEMPERATURE, IN A CONCENTRATED ELECTROLYTIC SOLUTION INCLUDING CHROMIC ACID AND SULFURIC ACID, SAID CONSTANT TEMPERATURE BEING BETWEEN 90* F. AND 120* F. SAID CHROMIC ACID BEING PRESENT IN CONCENTRATIONS RANGING FROM 40 TO 60 OUNCES PER GALLON OF SOLUTION; AND SAID SULFURIC ACID BEING PRESENT IN CONCENTRATIONS RANGING FROM 40 TO 60 OUNCES PER GALLON OF SOLUTION.

References Cited (Backward Citations)

US1144000A Cited
US1627900A Cited
US1923790A Cited
US1967716A Cited
GB465078A Cited
GB466949A Cited
US2580773A Cited
US2650901A Cited
US2662054A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1959-03-27 1959-09-26 1960-03-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1963-03-27 1963-09-26 1964-03-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1967-03-27 1967-09-26 1968-03-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag