Composite coated structural article

Assignee: Beazer East Inc
•
Filing: 1954-05-11
•
Granted: 1955-12-20
•
Expires: 1974-05-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 John C Christensen
  • 👤 Jr William F Fair

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 11:03
CPC Classifications
C; C04; C04B; C04B41/00; C04B41/45; C04B41/52; Y; Y10; Y10S; Y10S428/00; Y10S428/907; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31652

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 165 words
A PROCESS FOR RENDERING STRUCTURAL ARTICLES RESISTANT TO THE ATTACK OF PESTIFEROUS MARINE ORGANISMS AND TO CORROSION COMPRISING: APPLYING TO A STRUCTURAL ARTICLE A FIRST PROTECTIVE COATING OF A HOT COMPOSITION CONTAINING FROM ABOUT 65 TO ABOUT 80 PARTS BY WEIGHT OF COAL-TAR PITCH AND FROM ABOUT 20 TO ABOUT 35 PARTS BY WEIGHT OF FILLER; PERMITTING SAID FIRST PROTECTIVE COATING TO COOL AND HARDEN; APPLYING A SECOND COATING OF A FIBERED COAL-TAR PITCH EMULSION OVER SAID FIRST PROTECTIVE COATING, SAID FIBERED COAL-TAR PITCH EMULSION CONTAINING FROM ABOUT 77% TO ABOUT 81% BY WEIGHT OF COAL-TAR PITCH EMULSION, FROM ABOUT 3% TO ABOUT 9% BY WEIGHT OF MINERAL FIBERS, AND FROM ABOUT 11% TO ABUT 18% OF ADDED WATER; PERMITTING SAID SECOND COATING TO DRY; APPLYING A THIRD COATING OF A COMPOSITION COMPRISING FROM ABOUT 2 TO ABOUT 3 PARTS BY VOLUME OF SAND AND ABOUT 1 PART BY VOLUME OF PORTLAND CEMENT OVER SAID SECOND COATING; AND THEREAFTER PERMITTING SAID THIRD COATING TO HARDEN.
Claim 2
Dependent Claim 165 words
A PROCESS FOR RENDERING STRUCTURAL ARTICLES RESISTANT TO THE ATTACK OF PESTIFEROUS MARINE ORGANISMS AND TO CORROSION COMPRISING: APPLYING TO A STRUCTURAL ARTICLE A FIRST PROTECTIVE COATING OF A HOT COMPOSITION CONTAINING FROM ABOUT 65 TO ABOUT 80 PARTS BY WEIGHT OF COAL-TAR PITCH AND FROM ABOUT 20 TO ABOUT 35 PARTS BY WEIGHT OF FILLER; PERMITTING SAID FIRST PROTECTIVE COATING TO COOL AND HARDEN; APPLYING A SECOND COATING OF A FIBERED COAL-TAR PITCH EMULSION OVER SAID FIRST PROTECTIVE COATING, SAID FIBERED COAL-TAR PITCH EMULSION CONTAINING FROM ABOUT 77% TO ABOUT 81% BY WEIGHT OF COAL-TAR PITCH EMULSION, FROM ABOUT 3% TO ABOUT 9% BY WEIGHT OF MINERAL FIBERS, AND FROM ABOUT 11% TO ABUT 18% OF ADDED WATER; PERMITTING SAID SECOND COATING TO DRY; APPLYING A THIRD COATING OF A COMPOSITION COMPRISING FROM ABOUT 2 TO ABOUT 3 PARTS BY VOLUME OF SAND AND ABOUT 1 PART BY VOLUME OF PORTLAND CEMENT OVER SAID SECOND COATING; AND THEREAFTER PERMITTING SAID THIRD COATING TO HARDEN.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1958-12-19 1959-06-20 1959-12-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1962-12-19 1963-06-20 1963-12-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1966-12-19 1967-06-20 1967-12-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag