Abstract

No abstract record available.

Inventors

  • 👤 Richard G Clarke

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 05:08
CPC Classifications
C; C06; C06B; C06B45/00; C06B45/18; C06B45/30; C06B45/32; Y; Y10; Y10T; Y10T428/00; Y10T428/29

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 54 words
MAGNESIUM PARTICLES IN SUFFICIENTLY FINELY DIVIDED CONDITION AS TO BE READILY COMBUSTIBLE IN AIR AT ATMOSPHERIC PRESSURE AND TEMPERATURE, EACH OF SAID PARTICLES HAVING BEEN TREATED WITH DILUTE AMMONIUM HYDROXIDE OF ABOUT 0.9508 SP.GR. FOR ABOUT 30 TO 90 SECONDS FOLLOWED BY QUICK SEPARATION FROM THE AMMONIUM HYDROXIDE AND BY DRUING AT MODERATE TEMPERATURES
Claim 2
Dependent Claim 54 words
MAGNESIUM PARTICLES IN SUFFICIENTLY FINELY DIVIDED CONDITION AS TO BE READILY COMBUSTIBLE IN AIR AT ATMOSPHERIC PRESSURE AND TEMPERATURE, EACH OF SAID PARTICLES HAVING BEEN TREATED WITH DILUTE AMMONIUM HYDROXIDE OF ABOUT 0.9508 SP.GR. FOR ABOUT 30 TO 90 SECONDS FOLLOWED BY QUICK SEPARATION FROM THE AMMONIUM HYDROXIDE AND BY DRUING AT MODERATE TEMPERATURES
Claim 3
Dependent Claim 15 words
MAGNESIUM ACCORDING TO CLAIM 1, WHICH IS COATED WITH A THIN COATING OF A FUCHSONE.
Claim 4
Dependent Claim 86 words
THE PROCESS OF TREATING MAGNESIUM IN FINELY DIVIDED POWDER OR FLAKE FORM WHICH COMPRISES CONTACTING THE MAGNESIUM WITH AMMONIUM HYDROXIDE AQUEOUS SOLUTION OF WHICH ABOUT ONE-EIGHTH OF ITS WEIGHT IS NH3, CONTINUING THE CONTACT FOR ABOUT THIRTY TO NINETY SECONDS, SEPARATING THE AMMONIUM HYDROXIDE AND THE MAGNESIUM AS QUICKLY AS POSSIBLE, AND DRYING THE MAGNESIUM IN A LAYER NOT THICKER THAN ONE INCH AT A TEMPERATURE BETWEEN 150* F. AND 215* F., WHEREBY THE BURNING RATE OF THE MAGNESIUM IN OPEN AIR WILL BE SUBSTANTIALLY INCREASED.
Claim 5
Dependent Claim 86 words
THE PROCESS OF TREATING MAGNESIUM IN FINELY DIVIDED POWDER OR FLAKE FORM WHICH COMPRISES CONTACTING THE MAGNESIUM WITH AMMONIUM HYDROXIDE AQUEOUS SOLUTION OF WHICH ABOUT ONE-EIGHTH OF ITS WEIGHT IS NH3, CONTINUING THE CONTACT FOR ABOUT THIRTY TO NINETY SECONDS, SEPARATING THE AMMONIUM HYDROXIDE AND THE MAGNESIUM AS QUICKLY AS POSSIBLE, AND DRYING THE MAGNESIUM IN A LAYER NOT THICKER THAN ONE INCH AT A TEMPERATURE BETWEEN 150* F. AND 215* F., WHEREBY THE BURNING RATE OF THE MAGNESIUM IN OPEN AIR WILL BE SUBSTANTIALLY INCREASED.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1958-09-19 1959-03-21 1959-09-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1962-09-19 1963-03-21 1963-09-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1966-09-19 1967-03-21 1967-09-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag