← Back to Patent Explorer
US2689785A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for chemically polishing lead

Assignee: United States Department of the Navy
•
Filing: 1953-03-18
•
Granted: 1954-09-21
•
Expires: 1973-03-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Albert C Simon

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 13:35
CPC Classifications
C; C23; C23F; C23F3/00; C23F3/04; C23F3/06

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 162 words
A METHOD OF PRODUCING A POLISH OF HIGH LUSTER ON A LEAD SURFACE WHICH COMPRISES IMMERSING THE LEAD SURFACE IN CLEAN SMOOTH CONDITION INTO AN AQUEOUS POLISHING SOLUTION OF HYDROGEN PEROXIDE AND ACETIC ACID AND VIGOROUSLY AGITATING IT THEREIN FOR A TIME SUFFICIENT TO DEVELOP A POLISH OF HIGH LUSTER THEREON, QUICKLY WASHING THE POLISHING SOLUTION FROM THE LEAD SURFACE WITH AQUEOUS ACETIC ACID OF A CONCENTRATION NOT APPRECIABLY LESS THAN THAT OF THE POLISHING SOLUTION AND THEN WASHING THE LEAD SURFACE WITH WATER TO REMOVE THE ACETIC ACID, SAID POLISHING SOLUTION CONTAINING BETWEEN ABOUT 10 AND 25% BY WEIGHT HYDROGEN PEROXIDE AND BETWEEN ABOUT 15 AND 70% BY WEIGHT ACETIC ACID IN INVERSE PROPORTION AND IN A WEIGHT RATIO OF ACETIC ACID TO HYDROGEN PEROXIDE WHICH FOR EACH UNIT OF 5 WEIGHT PERCENT OF ACETIC ACID DECREASES WITH INCREASE IN THE HYDROGEN PEROXIDE CONTENT BY A FACTOR WHICH IS ABOUT 3.3% FOR EACH 1% INCREASE IN WEIGHT OF THE HYDROGEN PEROXIDE.
Claim 2
Independent Claim 162 words
A METHOD OF PRODUCING A POLISH OF HIGH LUSTER ON A LEAD SURFACE WHICH COMPRISES IMMERSING THE LEAD SURFACE IN CLEAN SMOOTH CONDITION INTO AN AQUEOUS POLISHING SOLUTION OF HYDROGEN PEROXIDE AND ACETIC ACID AND VIGOROUSLY AGITATING IT THEREIN FOR A TIME SUFFICIENT TO DEVELOP A POLISH OF HIGH LUSTER THEREON, QUICKLY WASHING THE POLISHING SOLUTION FROM THE LEAD SURFACE WITH AQUEOUS ACETIC ACID OF A CONCENTRATION NOT APPRECIABLY LESS THAN THAT OF THE POLISHING SOLUTION AND THEN WASHING THE LEAD SURFACE WITH WATER TO REMOVE THE ACETIC ACID, SAID POLISHING SOLUTION CONTAINING BETWEEN ABOUT 10 AND 25% BY WEIGHT HYDROGEN PEROXIDE AND BETWEEN ABOUT 15 AND 70% BY WEIGHT ACETIC ACID IN INVERSE PROPORTION AND IN A WEIGHT RATIO OF ACETIC ACID TO HYDROGEN PEROXIDE WHICH FOR EACH UNIT OF 5 WEIGHT PERCENT OF ACETIC ACID DECREASES WITH INCREASE IN THE HYDROGEN PEROXIDE CONTENT BY A FACTOR WHICH IS ABOUT 3.3% FOR EACH 1% INCREASE IN WEIGHT OF THE HYDROGEN PEROXIDE.

References Cited (Backward Citations)

US2446060A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1957-09-20 1958-03-22 1958-09-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1961-09-20 1962-03-22 1962-09-21 $3760.00 Window Closed / Lapsed