Age resisting nonstaining rubber composition and method of producing same

Assignee: Bridgestone Firestone Inc
•
Filing: 1950-07-01
•
Granted: 1953-07-28
•
Expires: 1970-07-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Joseph C Ambelang

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 16:58
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/04; C08K5/13; Y; Y10; Y10S; Y10S524/00; Y10S524/925

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 34 words
A RUBBER COMPOSITION RESISTANT TO DETERIORATION, COMPRISING VULCANIZED RUBBER CONTAINING A RELATIVELY SMALL AMOUNT OF THE REACTION PRODUCT OF 3 TO 4 MOLES OF FORMALDEHYDE AND 6 MOLES OF A DIALKYLPHENOL OF THE FORMULA
Claim 2
Dependent Claim 34 words
A RUBBER COMPOSITION RESISTANT TO DETERIORATION, COMPRISING VULCANIZED RUBBER CONTAINING A RELATIVELY SMALL AMOUNT OF THE REACTION PRODUCT OF 3 TO 4 MOLES OF FORMALDEHYDE AND 6 MOLES OF A DIALKYLPHENOL OF THE FORMULA

References Cited (Backward Citations)

GB622977A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1956-07-27 1957-01-26 1957-07-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1960-07-27 1961-01-26 1961-07-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1964-07-27 1965-01-26 1965-07-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag