Phenolic adhesive and method of bonding wood plies

Assignee: Weyerhaeuser Timber Co
•
Filing: 1944-12-26
•
Granted: 1951-11-13
•
Expires: 1964-12-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Clark C Heritage

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 04:23
CPC Classifications
C; C09; C09J; C09J161/00; C09J161/04; C09J161/06; C08; C08L; C08L2666/00; C08L2666/02; C08L2666/26; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31971; Y10T428/31975; Y10T428/31978; Y10T428/31982

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 76 words
AN ADHESIVE COMPOSITION COMPRISING A PHENOL-ALDEHYDE RESIN WHEREIN THE ALDEHYDE IS SELECTED FROM THE GROUP CONSISTING OF FORMALDEHYDE AND ACETALDEHYDE, AND AS AN ADHESIVE CONSTITUENT THE REACTION MASS RESULTING FROM CHEMICALLY REACTING COMMINUTED BARK, WATER AND ALKALI AT TEMPRATURES OF ABOUT 180* F., THE PROPORTION OF COMMINUTED BARK TO RESIN ON A DRY WEIGHT BASIS BEING WITHIN THE RANGE OF FROM 6 PARTS BARK TO 1 PART RESIN TO 2 PARTS BARK TO 6.5 PARTS RESIN.
Claim 2
Dependent Claim 76 words
AN ADHESIVE COMPOSITION COMPRISING A PHENOL-ALDEHYDE RESIN WHEREIN THE ALDEHYDE IS SELECTED FROM THE GROUP CONSISTING OF FORMALDEHYDE AND ACETALDEHYDE, AND AS AN ADHESIVE CONSTITUENT THE REACTION MASS RESULTING FROM CHEMICALLY REACTING COMMINUTED BARK, WATER AND ALKALI AT TEMPRATURES OF ABOUT 180* F., THE PROPORTION OF COMMINUTED BARK TO RESIN ON A DRY WEIGHT BASIS BEING WITHIN THE RANGE OF FROM 6 PARTS BARK TO 1 PART RESIN TO 2 PARTS BARK TO 6.5 PARTS RESIN.
Claim 3
Independent Claim 82 words
A METHOD FOR THE MANUFACTURE OF PLYWOOD, WHICH COMPRISES PREPARING AN ADHESIVE COMPOSITION COMPRISING AN ADMIXTURE OF A PHENOL-ALDEHYDE RESIN, WHEREIN THE ALDEHYDE IS SELECTED FROM THE GROUP CONSISTING OF FORMALDEHYDE AND ACETALDEHYDE, AND THE REACTION MASS RESULTING FROM REACTING WATER, AT LEAST ONE BASIC ACTING COMPOUND OF SODIUM, AND BARK POWDER, FORMING AN INTERFACE OF SAID COMPOSITION BETWEEN LAYERS OF WOOD VENEER TO BE UNITED, AND APPLYING HEAT AND PRESSURE TO THE SAID LAYERS AND INTERFACIAL COMPOSITION FOR SETTING THE ADHESIVE.
Claim 4
Independent Claim 82 words
A METHOD FOR THE MANUFACTURE OF PLYWOOD, WHICH COMPRISES PREPARING AN ADHESIVE COMPOSITION COMPRISING AN ADMIXTURE OF A PHENOL-ALDEHYDE RESIN, WHEREIN THE ALDEHYDE IS SELECTED FROM THE GROUP CONSISTING OF FORMALDEHYDE AND ACETALDEHYDE, AND THE REACTION MASS RESULTING FROM REACTING WATER, AT LEAST ONE BASIC ACTING COMPOUND OF SODIUM, AND BARK POWDER, FORMING AN INTERFACE OF SAID COMPOSITION BETWEEN LAYERS OF WOOD VENEER TO BE UNITED, AND APPLYING HEAT AND PRESSURE TO THE SAID LAYERS AND INTERFACIAL COMPOSITION FOR SETTING THE ADHESIVE.

References Cited (Backward Citations)

US118177A Cited
AU1244328A Cited
US1899768A Cited
US2068759A Cited
US2233875A Cited
US2319182A Cited
US2336672A Cited
US2314203A Cited
US2360376A Cited
US2380214A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1954-11-12 1955-05-14 1955-11-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1958-11-12 1959-05-14 1959-11-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1962-11-12 1963-05-14 1963-11-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag