Method for the production of viscose solutions

Assignee: Industrial Rayon Corp
•
Filing: 1946-07-18
•
Granted: 1950-07-04
•
Expires: 1966-07-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Kline Emil

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 20:50
CPC Classifications
D; D01; D01F; D01F2/00; D01F2/06; D01F2/08

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 161 words
IN THE PROCESS OF FORMING A VISCOSE SOLUTION IN WHICH PROCESS A QUANTITY OF ALKALI CELLULOSE HAVING AN ALKALINITY OF THE ORDER OF ABOUT 15% NAOH BY WEIGHT IS INTRODUCED INTO A CHURN AND TREATED WITH CARBON DISULFIDE TO FORM SODIUM CELLULOSE XANTHATE AND IN WHICH AN AQUEOUS CAUSTIC SODA SOLUTION IS THEREAFTER ADMIXED WITH SAID FORMED CELLULOSE XANTHATE AND THE MIXTURE DISCHARGED INTO A DISSOLVING VESSEL TO FORM A FISCOSE SOLUTION THE STEPS COMPRISING; SCAVENGING SAID DISCHARGED CHURN AT LEAST ONCE WITH AN AQUEOUS CAUSTIC SODA SOLUTION HAVING AN ALKALINITY LESS THAN THAT OF SAID ALKALI CELLULOSE; DISCHARGING SAID SCAVENGING SOLUTION FROM SAID CHURN; COMBINING IN A DISSOLVING VESSEL SUBSTANTIALLY ALL OF SAID DISCHARGED SCAVENGING SOLUTION WITH AID PREVIOUSLY DISCHARGED MIXTURE TO FORM A VISCOSE SOLUTION HAVING AN ALKALINITY BETWEEN ABOUT 5% AND 8% NAOH BY WEIGHT; THEREAFTER INTRODUCING ANOTHR QUANTITY OF ALKALI CELLULOSE INTO SAID CHURN WHILE SAID CHURN IS STILL WET WITH SCAVENGING SOLUTION; AND REPEATING THE CYCLE.
Claim 2
Dependent Claim 161 words
IN THE PROCESS OF FORMING A VISCOSE SOLUTION IN WHICH PROCESS A QUANTITY OF ALKALI CELLULOSE HAVING AN ALKALINITY OF THE ORDER OF ABOUT 15% NAOH BY WEIGHT IS INTRODUCED INTO A CHURN AND TREATED WITH CARBON DISULFIDE TO FORM SODIUM CELLULOSE XANTHATE AND IN WHICH AN AQUEOUS CAUSTIC SODA SOLUTION IS THEREAFTER ADMIXED WITH SAID FORMED CELLULOSE XANTHATE AND THE MIXTURE DISCHARGED INTO A DISSOLVING VESSEL TO FORM A FISCOSE SOLUTION THE STEPS COMPRISING; SCAVENGING SAID DISCHARGED CHURN AT LEAST ONCE WITH AN AQUEOUS CAUSTIC SODA SOLUTION HAVING AN ALKALINITY LESS THAN THAT OF SAID ALKALI CELLULOSE; DISCHARGING SAID SCAVENGING SOLUTION FROM SAID CHURN; COMBINING IN A DISSOLVING VESSEL SUBSTANTIALLY ALL OF SAID DISCHARGED SCAVENGING SOLUTION WITH AID PREVIOUSLY DISCHARGED MIXTURE TO FORM A VISCOSE SOLUTION HAVING AN ALKALINITY BETWEEN ABOUT 5% AND 8% NAOH BY WEIGHT; THEREAFTER INTRODUCING ANOTHR QUANTITY OF ALKALI CELLULOSE INTO SAID CHURN WHILE SAID CHURN IS STILL WET WITH SCAVENGING SOLUTION; AND REPEATING THE CYCLE.

References Cited (Backward Citations)

US1807370A Cited
GB456841A Cited
US2338196A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1953-07-03 1954-01-02 1954-07-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1957-07-03 1958-01-02 1958-07-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1961-07-03 1962-01-02 1962-07-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag