Optical part molding material
Abstract
Abstract PURPOSE: To obtain an optical part molding material useful as a substrate for application type optical disc, having excellent transparency, heat resistance and chemical resistance, comprising a polyvinylcyclohexane polymer prepared by hydrogenating an aromatic ring of styrene polymer. CONSTITUTION: The aromatic ring of a styrene polymer (styrene homopolymer or copolymer containing ≥60wt.% styrene and one or more monomers copolymerizable with styrene) is hydrogenated in the presence of a hydrogenating catalyst such as Raney nickel or ruthenium supported on carbon or alumina under 50W250Kg/cm 2 at 100W200°C for 0.5W5hr to give the aimed material comprising a polyvinylcyclohexane polymer. The polymer is heated and dried, water in the polymer is removed to prevent formation of foams and the polymer is molded usually at 230W350°C to give a molded article suitable for optical uses, having excellent transparency and small strain. COPYRIGHT: (C)1989,JPO&Japio
Inventors
- 👤 Seiichi Mukai
- 👤 Ryoko Kojika
- 👤 Mikiro Nakazawa
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
Maintenance schedule is calculated for granted US utility patents.