← Back to Patent Explorer
JPS6086243A Expired / Lapsed JP ⏱️ 0.0 years remaining

Abrasion resistance roll

Assignee: Nippon Steel Corp
•
Filing: 1983-10-18
•
Granted: —
•
Expires: 2003-10-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract PURPOSE:To prepare an abrasion resistant roll having high hardness, by applying the build-up welding of a hard metal having a specific composition based on C- Cr to the surface of a hot rolled roll before applying nitrification treatment thereto. CONSTITUTION:A hard low alloyed steel layer having a specific composition is formed to the surface of a hot rolled roll by build-up welding. That is, steel containing 0.10-0.50% C, 0.20-2.0% Si, 0.30-3.0% Mn, 0.5-4.0% Cr and at least one of 0.01-0.20% Ti and 0.002-0.20% B or steel prepared further containing one or more of Mo<4.0%, V<2.0%, Al<2.0% and Nb<2.0% in the former steel is subjected to build-up welding. The build-up layer having fine hard carbide is subjected to nitrification treatment due to an ammonia gas nitrification method to make it possible to prepare a roll having extremely high hardness and excellent abrasion resistance.

Inventors

  • 👤 Hiroyuki Koike
  • 👤 弘之 小池
  • 👤 Hitoshi Nishimura
  • 👤 西村 均

Bibliographic Details

Application Number —
Jurisdiction JP
Data Source google_patents
Last Synchronized 2026-11-09 13:35
CPC Classifications
—

Claims Analysis

Total Claims: 0
No claims parsed yet. Click Sync Now above to re-index claims from Google Patents.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag