Adhesion of fluoric resin
Abstract
Abstract PURPOSE:To securely adhere fluoric resin products together at a high strength in a short time by such an arrangement wherein the surface of a fluoric resin product to which other is adhered is treated by corona discharge and epoxy resin is used as a primer and thermoplastic polyester is used as an adhesive. CONSTITUTION:Fluoric resin products are adhered together by such a method wherein the surface of a fluoric resin product (preferably, copolymer resin of tetrafluoroethylene-ethylene shown by the formula) to which other product is adhered is treated by corona discharge, and epoxy resin (preferably, bisphenol A type epoxy resin of which epoxy equivalent is more than 800) is coated on the surface under such baking conditions preferably as 150-200 deg.C and for 10sec- 30min as a primer so that its film thickness becomes 5-300mg/dm<2>, and as an adhesive, thermoplastic polyester (preferably, one of which melting temperature is 80-200 deg.C and reduction viscosity is 0.2-1.0g/dl) or polyamide (preferably, one of which melting temperature is 80-200 deg.C and relative viscosity is 1.3- 2.0) is used.
Inventors
- 👤 Sukeyuki Ishibashi
- 👤 石橋 祐之
- 👤 Kunio Tawara
- 👤 邦夫 俵
- 👤 Yoshiaki Fujimoto
- 👤 藤本 嘉明
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
Maintenance schedule is calculated for granted US utility patents.