Wet forming method for fine zinc oxide

Assignee: Dowa Holdings Co Ltd
•
Filing: 1978-09-22
•
Granted: —
•
Expires: 1998-09-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract PURPOSE: To produce fine zinc oxide of uniform shape by neutralizing or heating a basic zinc salt formed by neutralizing an aq. soln. contg. a zinc salt. CONSTITUTION: An aq. soln. of a zinc salt such as zinc nitrate is neutralized with an alkali agent such as NH 3 or NaOH at such a relatively low temp. as below 80°C to convert part or most of the zinc salt into a basic zinc salt such as basic zinc nitrate once. The aq. soln. is further neutralized at the relatively low temp. to finallly form zinc oxide. The basic zinc salt may be formed at low temp. io a low pH value and decomposed by heating optionally after separating the mother liquor. Thus, zinc oxide of 1μ or below in grain size is stably obtd., and the grain size and shape of the zinc oxide are uniform. COPYRIGHT: (C)1980,JPO&Japio

Inventors

  • 👤 Seiichi Kuno

Bibliographic Details

Application Number —
Jurisdiction JP
Data Source google_patents
Last Synchronized 2026-11-02 19:24
CPC Classifications
—

Claims Analysis

Total Claims: 0
No claims parsed yet. Click Sync Now above to re-index claims from Google Patents.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag