Abstract

Abstract Improved autodeposited coatings on metallic surfaces are formed by contacting the metallic surfaces with an autodepositing composition comprising an acidic aqueous coating solution containing dispersed solid resin particles of either an internally stabilized or externally stabilized vinylidene chloride polymer, an exemplary internally stabilized polymer being prepared from vinylidene chloride and a monomeric surfactant which includes an inorganic ionizable group, and an exemplary externally stabilized poly er being prepared from vinylidene chloride and a reactive comonomer, the resulting resin particles having surfactant adsorbed thereon, said autodeposited coatings having extremely good corrosion resistant properties without treatment with a reaction rinse such as a chromium rinse. Curing of autodeposited coatings of various types, including those mentioned above, by treatment with water or steam is disclosed also.

Inventors

  • 👤 Wilbur S. Hall
  • 👤 Bashir M. Ahmed

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-11-05 15:54
CPC Classifications
C; C08; C08F; C08F214/00; C08F214/02; C08F214/04; C08F214/08; B; B05; B05D; B05D7/00; B05D7/14; B05D7/142; B05D7/144; C09; C09D; C09D5/00; C09D5/08; C09D5/088

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 28 words
A process for curing an autodeposited coating compri­sing subjecting an uncured autodeposited coating to steam or water having a temperature of about 21°C (70°F) to about 100°C (212°F).
Claim 2
Dependent Claim 28 words
A process for curing an autodeposited coating compri­sing subjecting an uncured autodeposited coating to steam or water having a temperature of about 21°C (70°F) to about 100°C (212°F).
Claim 3
Dependent Claim 26 words
A process according to Claim 1 wherein said coating is cured by immersion in water at a temperature of about 21°C (70°F) to about 100°C (212°F).
Claim 4
Dependent Claim 16 words
A process according to Claim 1 wherein said coating is cured by treating it with steam.
Claim 5
Dependent Claim 32 words
A process according to Claim 1 including rinsing residuals from said coating and curing said coating simul­taneously by spraying said coating with hot water or immersing it into a hot water bath.
Claim 6
Dependent Claim 35 words
A process according to Claim 1 wherein said coating is cured for a period of time of about 5 seconds to about 5 minutes at a temperature of about 85°C (185°F) to about 100°C (212°F).
Claim 7
Dependent Claim 21 words
A process according to Claim 5 wherein said period of time is no longer than about 2 to about 3 minutes.
Claim 8
Dependent Claim 36 words
A process according to Claim 1 wherein said coating is immersed into water having a temperature of about 85°C (185°F) to about 100°C (212°F) for a period of time of about 5 to about 30 seconds.
Claim 9
Dependent Claim 29 words
A process according to Claim 1, 2, 3, 4, 5, 6 or 7 wherein said coating comprises a resin having a Tg of no greater than about 60°C (140°F).
Claim 10
Dependent Claim 30 words
A process according to Claim 1, 2, 3, 4, 5, 6, 7 or 8 wherein said coating comprises a resin having a Tg of no greater than about 37.7°C (100°F).
Claim 11
Dependent Claim 30 words
A process according to Claim 1, 2, 3, 4, 5, 6, 7 or 8 wherein said coating comprises a resin having a Tg of no greater than about 29.4°C (85°F).
Claim 12
Dependent Claim 13 words
A process according to Claim 3 wherein said steam is at atmospheric pressure.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag