Abstract

Abstract A method for providing fibrous polyamide materials with stain resistance is provided. The method comprises contacting the fibrous polyamide materials with an aqueous solution comprising a normally solid, water-soluble, partially sulfonated novolak resin, which comprises the condensation product of at least one phenolic compound and an aldehyde, and a water-soluble divalent metal salt.

Inventors

  • 👤 George L. C/O Minnesota Mining And Payet
  • 👤 John Cheng-Chung C/O Minnesota Mining And Chang

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-10-31 21:41
CPC Classifications
D; D06; D06M; D06M15/00; D06M15/19; D06M15/37; D06M15/39; D06M15/41; D06M15/412

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 49 words
A method for providing fibrous polyamide materials with stain resistance comprising contacting the fibrous polyamide materials with an aqueous solution comprising a normally solid, water-soluble, partially sulfonated novolak resin, which comprises the condensation product of at least one phenolic compound and an aldehyde, and a water-soluble divalent metal salt.
Claim 2
Independent Claim 49 words
A method for providing fibrous polyamide materials with stain resistance comprising contacting the fibrous polyamide materials with an aqueous solution comprising a normally solid, water-soluble, partially sulfonated novolak resin, which comprises the condensation product of at least one phenolic compound and an aldehyde, and a water-soluble divalent metal salt.
Claim 3
Dependent Claim 89 words
The method of claim 1 comprising adding to a dyebath, before, during or after dyeing of the polyamide material, at least 0.1% solids based on the weight of the polyamide material of said sulfonated novolak resin and at least 1% based on the weight of the polyamide material of said water-soluble divalent metal salt, immersing the polyamide material in the dyebath for a time and temperature sufficient to exhaust the sulfonated novolak resin onto the polyamide material, removing the polyamide material from the dyebath and drying the polyamide material.
Claim 4
Dependent Claim 74 words
The method of claim 1 comprising applying to the polyamide material a solution comprising at least 0.1% solids based on the weight of the polyamide material of said sulfonated novolak resin and at least 1% of said water-soluble divalent metal salt based on the weight of the polyamide material, steaming said polyamide material for a time sufficient to effect adherence of said sulfonated novolak resin to said polyamide material, and drying the polyamide material.
Claim 5
Dependent Claim 50 words
The method of claim 1 comprising padding a solution comprising at least 0.1% based on the weight of the polyamide material of said sulfonated novolak resin and 1% based on the weight of the polyamide material of said divalent metal salt onto the polyamide material and drying he polyamide material.
Claim 6
Dependent Claim 24 words
The method of claim 1 wherein said water-soluble, divalent metal salts are selected from inorganic and organic salts of magnesium, barium, calcium, and zinc.
Claim 7
Dependent Claim 24 words
The method of claim 1 wherein said sulfonated novolak resin comprises a sulfonated condensation product of at least one phenolic compound and an aldehyde.
Claim 8
Dependent Claim 27 words
The method of claim 1 wherein said aqueous solution further contains a fluorochemical oil and water repellent composition and said water-soluble metal salt is a magnesium salt.
Claim 9
Dependent Claim 12 words
A fibrous polyamide material treated according to the method of claim 1.
Claim 10
Dependent Claim 28 words
An aqueous solution for providing stain resistance to fibrous polyamide materials, said solution comprising a normally solid, water-soluble, partially sulfonated novolak resin and a water-soluble divalent metal salt.
Claim 11
Dependent Claim 28 words
An aqueous solution for providing stain resistance to fibrous polyamide materials, said solution comprising a normally solid, water-soluble, partially sulfonated novolak resin and a water-soluble divalent metal salt.
Claim 12
Dependent Claim 44 words
The solution of claim 9 wherein said solution comprises at least 0.1% solids based on the weight of the polyamide material of said sulfonated novolak resin and at least 1% of said water-soluble divalent metal salt based on the weight of the polyamide material.
Claim 13
Dependent Claim 17 words
The solution of claim 9 wherein said solution further comprises a fluorochemical oil and water repellent composition.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag